Re: Drop with Dropring

Hi, Jan. My wife and I have made a lot of drop vases, many of them using a 9-inch ring that is similar to yours in size, but is made of ceramic. Is your metal ring one solid piece? I ask because metal generally shrinks more than glass as it cools, so I worry that the ring might trap your vase. We us...
by michaelmace
Mon Aug 17, 2020 2:21 pm
Forum: Newcomer Forum
Topic: I think I have a bad relay. Am I doing this right?
Replies: 3
Views: 11279

I think I have a bad relay. Am I doing this right?

Hi, gang. I’m a new poster here, but have been lurking for years and deeply appreciate all of the wisdom posted here. I think I have a bad relay in my kiln, but wanted to check with the experts to make sure I didn’t overlook any other potential problems. I have a Paragon Janus 1613, which is a hybri...