- Mon Oct 16, 2023 2:43 pm
- Forum: Techniques and Tools
- Topic: Slump breakage
- Replies: 1
- Views: 17172
Slump breakage
All spectrum (96coe) used. Same schedule as used before and other pieces in kiln were fine. When lifted out of mold end pieces broke. Don’t think it is incompatibility since all labeled 96. What else could it be?
- Mon Apr 17, 2023 4:32 pm
- Forum: Techniques and Tools
- Topic: Modifying a slumping mold
- Replies: 4
- Views: 4254
Re: Modifying a slumping mold
Fiber paper is so thin I don’t know how I would get any raised fluted shape. Is there something to build up the surface under the fiber paper?
Thanks!
Thanks!
- Mon Apr 17, 2023 2:43 pm
- Forum: Techniques and Tools
- Topic: Modifying a slumping mold
- Replies: 4
- Views: 4254
Modifying a slumping mold
I have a large (20”) ball mold I would like to make undulate on the side surface. It would only need a few areas bumped in to make it more organic. Can this be done with fiber paper or ???
Thanks, Linda