Search found 4 matches
- Tue Nov 10, 2020 7:25 am
- Forum: Techniques and Tools
- Topic: Coke & Corona Bottle Slump
- Replies: 8
- Views: 34131
Re: Coke & Corona Bottle Slump
Thank You So Much! I’ll try a new schedule & see what happens!
- Mon Nov 09, 2020 3:12 pm
- Forum: Techniques and Tools
- Topic: Coke & Corona Bottle Slump
- Replies: 8
- Views: 34131
Re: Coke & Corona Bottle Slump
Thanks for your input! Just curious, why 1,000 instead of 950?
Also, sometimes I peek in (I can’t see much, it’s a tiny window) & my bottle has already slumped before step 3,,, so maybe I do need a lower temp in 1/2
Also, sometimes I peek in (I can’t see much, it’s a tiny window) & my bottle has already slumped before step 3,,, so maybe I do need a lower temp in 1/2
- Sun Nov 08, 2020 10:51 pm
- Forum: Techniques and Tools
- Topic: Coke & Corona Bottle Slump
- Replies: 8
- Views: 34131
Re: Coke & Corona Bottle Slump
I’ve been using:
1-500°,1100°,10
2-250°,1300°, 5
3-300°,1425°, 5
4-full, 950°, 40
1-500°,1100°,10
2-250°,1300°, 5
3-300°,1425°, 5
4-full, 950°, 40
- Sun Nov 08, 2020 2:05 pm
- Forum: Techniques and Tools
- Topic: Coke & Corona Bottle Slump
- Replies: 8
- Views: 34131
Coke & Corona Bottle Slump
Hi, I’m totally new to bottle slumping & I was wondering what I am doing wrong that my painted Coca Cola labels burn completely off of the back, while the red burns off of the front leaving only the white. Meanwhile, my painted Corona labels stay on in the front but the back labels burn into my ...