Hydrocal Hell
Hello, I have not been able to find an answer and I'm hoping the forum can help: I am in the process of making a pate de verre box. The folks at Bullseye said that I would be able to use straight Hydrocal for my plaster mold. In Boyce Lundstrom's book he said to take the mold to 1200 degrees to burn...