Search found 2 matches

by mktucker
Wed Sep 03, 2003 8:45 pm
Forum: Techniques and Tools
Topic: kiln questions
Replies: 4
Views: 8316

Thanks all for the info, I have an Olympic 189GFE, decided not to start with the tabletop type as I knew I would end up buying a second kiln. I hope to also do some pottery later but for now the glass fusing has my interest. I've done about 20 jewelry pieces so far and no cracks but plan to move on ...
by mktucker
Tue Sep 02, 2003 7:51 pm
Forum: Techniques and Tools
Topic: kiln questions
Replies: 4
Views: 8316

kiln questions

I'm new to to this fusing and have a kiln that will temp up fairly quickly, how fast can I do simple fusing of bullseye, and can I just let it cool naturally once it is flashed to about l000? I can program the kiln if necessary but I hate to add unnecessary steps. I'm trying to learn on my own plus ...