- Fri Jul 23, 2021 11:37 am
- Forum: Kiln Casting
- Topic: Power failure
- Replies: 1
- Views: 18711
Power failure
We had a power failure during my kiln firing. The kiln was at the annealing stage approching and very close to 880 goal point and scheduled to hold for 2 hours. It had been droping 6 degrees per hour from 990 for the past 10 hours. It was to hold for 2 hours at 880 before going to the 600 soak for a...