Search found 1 match
- Mon Mar 07, 2022 11:52 am
- Forum: Techniques and Tools
- Topic: Slumping a double curve mould
- Replies: 1
- Views: 3190
Slumping a double curve mould
Hi you bunch of geniuses! I'm just about to slump a piece of bullseye glass which is 3mm thick 10" x 6" and has been fused with frit powders. How long should the ramp time be and to what temperature? Sorry to ask such an obvious question but I am mystified & very nervous as its my firs...