Search found 168 matches
- Mon Sep 22, 2014 12:56 pm
- Forum: Business Topics
- Topic: Designing a new studio
- Replies: 38
- Views: 61921
Re: Designing a new studio
Marty, my cold shop is missing a very serviceable item: it's lacking a cold-working table with shallow sides, rubber matting, with a built in drain, for washing, rinsing, and angle grinding. Bullseye at Portland have one and use it with their Suhner rotifera; another tool to die for. Might also want...
- Fri Jun 13, 2014 9:18 pm
- Forum: Kiln Casting
- Topic: Dental plaster
- Replies: 17
- Views: 31200
Re: Dental plaster
Great!! info. But please be clear: quatz vs quarts; alumina vs aluminum. Lots of confusion could arise.
Cheers
Cheers
- Thu Apr 17, 2014 12:20 pm
- Forum: Photos and Stuff
- Topic: Blankets X 2
- Replies: 15
- Views: 22174
Re: Blankets X 2
Kudos! Two grey hills design
is especially beautiful.
is especially beautiful.
- Tue Jan 07, 2014 3:05 pm
- Forum: Techniques and Tools
- Topic: Glue for fused work
- Replies: 24
- Views: 42435
Re: Glue for fused work
Rave (pump, not aerosol) hairspray works well.
- Tue Nov 19, 2013 5:20 pm
- Forum: Photos and Stuff
- Topic: The Wentworth Bartop
- Replies: 13
- Views: 18524
Re: The Wentworth Bartop
Beautiful; congratulations!
Nikki
Nikki
- Sat Oct 12, 2013 6:16 pm
- Forum: Techniques and Tools
- Topic: Dictionary
- Replies: 29
- Views: 35783
Re: Dictionary
Randy, spot on.. My husband doesn't' understand why I go to bed reading Charles's dictionary...such a wealth of info. A tome for glass. So much there. But for a a more recent vernacular, it would be useful for definitions for currant usages for glass terms. It's surely a problem across various arts ...
- Sat Oct 12, 2013 4:27 pm
- Forum: Techniques and Tools
- Topic: Dictionary
- Replies: 29
- Views: 35783
Re: Dictionary
A first iteration in English, followed by translations,would save time, I think.
Terms and meanings as they are actually used is a great idea. Brad has gone a long way already.
Nikki
Terms and meanings as they are actually used is a great idea. Brad has gone a long way already.
Nikki
- Tue Aug 06, 2013 8:05 pm
- Forum: Photos and Stuff
- Topic: New Powder Paintings - Landscapes
- Replies: 14
- Views: 18814
Re: New Powder Paintings - Landscapes
Your second landscape is simply magnificent. the way you handled light is mesmerizing. Good job! Lots to explore here.
Nikki
Nikki
- Mon Jul 22, 2013 7:40 pm
- Forum: Kiln Casting
- Topic: New Book
- Replies: 7
- Views: 12806
Re: New Book
Angela's book is great; a fairly thorough compilation and synthesis of her PhD thesis work. Lots of nuggets there. The CD is a tome to wade through that would be of interest to dedicated casters.
Nikki
Nikki
- Mon Jul 22, 2013 7:32 pm
- Forum: Techniques and Tools
- Topic: Karl Harron 3 step mold
- Replies: 7
- Views: 11379
Re: Karl Harron 3 step mold
Heat work; because it doesn't take as long to get there ?
- Sat Jun 08, 2013 7:55 pm
- Forum: Photos and Stuff
- Topic: Three panels for a home
- Replies: 21
- Views: 26378
Re: Three panels for a home
Stuningly beautiful work, Don. Great stuff.
Nikki
Nikki
- Thu Mar 14, 2013 8:08 am
- Forum: Techniques and Tools
- Topic: Lap Grinder
- Replies: 14
- Views: 16634
Re: Lap Grinder
Take a look at ASW's 18 and 24" flat laps. The 24" one I have has given me no problems for 8 years now, and disks are easy to change (unlike some brands). Water comes up the center. For quality, get disks from HIS, not ASW. A friend has the 18"; delightful.
- Fri Feb 01, 2013 9:53 pm
- Forum: Photos and Stuff
- Topic: Light Reading
- Replies: 16
- Views: 18326
Re: Light Reading
Bob I can't believe they wouldn't find a quiet place for this stack of books. They have a lovely spirit, and would be a special surprise when visitors come upon them. that is, of course, if you would possible want to let them go. I was looking at images of Ron's boxes yesterday. I miss his creative ...
- Fri Feb 01, 2013 9:46 pm
- Forum: Photos and Stuff
- Topic: Colors and Abstraction for Leslie
- Replies: 6
- Views: 8387
Re: Colors and Abstraction for Leslie
Lusciously yummy! Nice job.
Nikki
Nikki
- Mon Dec 10, 2012 11:49 pm
- Forum: Techniques and Tools
- Topic: Edges on Bowls
- Replies: 2
- Views: 3987
Re: Edges on Bowls
Talk to the people at Covington. A rociprolap machine is not what you want. A flat lap machine is what is usually used to achieve a flat lip that is parallel to the base. Also check out ASW flat lap machines in California, and flat lap disks by HIS Glassworks, as well as their informative videos. So...
- Mon Dec 10, 2012 11:21 pm
- Forum: Photos and Stuff
- Topic: Glilt Trip
- Replies: 18
- Views: 23009
Re: Glilt Trip
Bob, it's such a beautifully rich and quiet piece! The texture and design seem to exude good feelings about home and craft and life. No wonder it sold so quickly. Congratulations to Liesbeth on this new venture. Hope you tow do more together.
Hugs,
Nikki
Hugs,
Nikki
- Mon Dec 03, 2012 9:05 pm
- Forum: Photos and Stuff
- Topic: Cave Art
- Replies: 17
- Views: 16783
Re: Cave Art
Babette, you might want to send Bob an email. Maybe he would have some insight. The paleolithic horse I made in his class is as special as the piece you expanded upon to make, and hopefully your piece will find a home on a wall in your house.
Cheers,
Nikki
Cheers,
Nikki
- Mon Dec 03, 2012 5:13 pm
- Forum: Photos and Stuff
- Topic: Cave Art
- Replies: 17
- Views: 16783
Re: Cave Art
Babette: It sure looks and sounds like incompatibility with white. Nice piece. You could try blast away the cracks if they aren't all the way through, and pumice. Or cut up the piece in sections and re-assemble leaving out the cracked areas.
Nikki
Nikki
- Thu Nov 29, 2012 12:03 pm
- Forum: Jewelry Making
- Topic: rubber tubing
- Replies: 4
- Views: 10083
Re: rubber tubing
Doug, for "traditional" findings "Rio Grand offers a huge catalog. Have jun with the new venture.
Nikki
Nikki
- Mon Oct 08, 2012 3:22 pm
- Forum: Kiln Casting
- Topic: US equivalent for Keramicast
- Replies: 9
- Views: 15850
Re: US equivalent for Keramicast
Cynthia, thanks for the tips and reminders! We met at BCon at the pate de vere and casting conference and talked a bit about mold making. Everything you said resonates. It's a bit of work (and fun) to instill or re-instill casting and mold making details back into the brain, after not having done an...