Re: plaster silica

Speaking of old plaster, I have a sealed box of C & R Loo MM 522 from 17 years ago, that I never got around to using (or opening). I have no idea what the mold mix is but would like to use it...part of finding and clearing out obsolete stuff and starting fresh. What else to do while hibernating?...
by Nikki ONeill
Mon Sep 28, 2020 10:27 am
Forum: Techniques and Tools
Topic: Light weight Kiln Shelf
Replies: 7
Views: 5211

Re: Light weight Kiln Shelf

I've used the high density vermiculite board in my GL 44 kiln for about 10 years. The board measures about 19 X 40", 1" thick, and kilnwashed. Hasn't warped yet. Originally sourced from Skamol (HD 60 as I recall) but now available from Bullseye. For smaller work, I elevate it on the sides ...
by Nikki ONeill
Mon Aug 05, 2019 10:16 am
Forum: Kiln Casting
Topic: Mold Mix 6
Replies: 5
Views: 8823

Re: Mold Mix 6

Good idea. thanks Leslie!
by Nikki ONeill
Mon Aug 05, 2019 9:01 am
Forum: Kiln Casting
Topic: Mold Mix 6
Replies: 5
Views: 8823

Re: Mold Mix 6

Thank You Leslie for the wonderfully presented video. Clear, excellent instructions. I want to mention that I took my rock solid sample and immersed it in water for a day and it became workable. Mixing with a hand mixer made it creamy again. I hope the fibers are still in good shape!
by Nikki ONeill
Sun Jan 13, 2019 6:18 pm
Forum: Techniques and Tools
Topic: irritating news
Replies: 11
Views: 9346

Re: irritating news

Welcome back, friend. Glad you';re on the mend! I'm in week 5 after hip replacement and doing well too. I finished and shipped out two commissions the day before surgery, and during recovery dreamed up all kinds of new pieces. Do report on your new works.
by Nikki ONeill
Wed Apr 25, 2018 11:49 am
Forum: Photos and Stuff
Topic: Another...recent work
Replies: 9
Views: 10687

Re: Another...recent work

I do remember those days :-). It will be fun to get together. I'm slated to teach at Warren Nyggard's studio, Milkweed Arts. My "Corallite Creations" class is not advertised there yet, but we're planning for a 4 day class, March 15-18. Let me know if you'll be available for a visit during ...
by Nikki ONeill
Mon Apr 23, 2018 12:18 pm
Forum: Photos and Stuff
Topic: Another...recent work
Replies: 9
Views: 10687

Re: Another...recent work

Beautiful work! Its a trip down memory lane to see those maglesses. I have one of your postcards, Jim, plus your sweet magless. Your post card sits on my windowsill in the workshop, alongside the orange tree miniature. Can I come by and visit you in Phoenix next March? I'll be teaching my Corallite ...
by Nikki ONeill
Mon Apr 23, 2018 11:53 am
Forum: Techniques and Tools
Topic: Two layer vase
Replies: 7
Views: 5910

Re: Two layer vase

Michele, how about one sheet most of the way, annealing and cooling, then adding the second sheet and slump again. there might be would be less chance or fewer places for layers to stick to each other.
by Nikki ONeill
Sun Feb 25, 2018 1:12 pm
Forum: Photos and Stuff
Topic: glass I'm working on
Replies: 20
Views: 23537

Re: glass I'm working on

Lovely work, Don.
by Nikki ONeill
Mon Jan 29, 2018 12:20 pm
Forum: Kiln Casting
Topic: Mold Mix 6
Replies: 5
Views: 8823

Mold Mix 6

I have a couple unopened samples of Zircar's Mold Mix 6, and they are almost rock solid. Has anyone tried to reconstitute this material with a little water and perhaps a blender? According to Zircar, it might not be worth the effort. I want to paint some on a mold made from Zircar sheet material, fo...
by Nikki ONeill
Wed Dec 21, 2016 8:17 pm
Forum: Photos and Stuff
Topic: Prickly Pear Suncatcher
Replies: 9
Views: 10206

Re: Prickly Pear Suncatcher

Beautiful, Don.

I brought out my four treasures you made a few years ago, to show my grandchildren: polar bear, rabbits, chipmunk, and a big mouse? with along tail. The two and four-year-olds were captivated! Too precious to hang on the tree, we put them on a window sill.
Cheers!
by Nikki ONeill
Wed Mar 09, 2016 3:12 pm
Forum: Techniques and Tools
Topic: Slumping into the smaller deep bowl mold set
Replies: 2
Views: 4055

Re: Slumping into the smaller deep bowl mold set

Babette, the website for the molds, descriptions, and suggested firing schedules is on the Creative Ceramics.com website. They list the molds under "new" and the three are called Bowl 2, step I, II, and III. Bowl 2 step 1 mold is similar to the regular ball molds that Bullseye stocks but a...
by Nikki ONeill
Mon Mar 07, 2016 9:32 pm
Forum: Techniques and Tools
Topic: Slumping into the smaller deep bowl mold set
Replies: 2
Views: 4055

Slumping into the smaller deep bowl mold set

Does anyone have experience slumping in Creative Ceramic's smaller deep vessel set of three molds? Bullseye sells them on special order. There is an inner and outer wall on the second and third mold. Has anyone tried manipulating these in the kiln during the slump? Seems the design would insulate th...
by Nikki ONeill
Tue Jan 12, 2016 9:54 am
Forum: Techniques and Tools
Topic: Stainless Steel for molds?
Replies: 15
Views: 19878

Re: Stainless Steel for molds?

Bert, don't you mean that ss shrinks more than glass, thus the potential of a ss mold trapping the glass? I've not has a problem unless the ss mold is a full hemisphere.
by Nikki ONeill
Fri Aug 14, 2015 9:17 pm
Forum: Techniques and Tools
Topic: metal spinning company
Replies: 1
Views: 3438

Re: metal spinning company

Thanks, Rosanna
Cheers,
Nikki
by Nikki ONeill
Sat Jan 31, 2015 10:40 pm
Forum: Photos and Stuff
Topic: Books from the Light Reading series
Replies: 14
Views: 14267

Re: Books from the Light Reading series

Gorgeous, precious, and thoughtful books, especially the songbook with the birds on the front seeming to communicate. Kudos again, Bob.
Nikki
by Nikki ONeill
Mon Sep 22, 2014 12:56 pm
Forum: Business Topics
Topic: Designing a new studio
Replies: 38
Views: 38195

Re: Designing a new studio

Marty, my cold shop is missing a very serviceable item: it's lacking a cold-working table with shallow sides, rubber matting, with a built in drain, for washing, rinsing, and angle grinding. Bullseye at Portland have one and use it with their Suhner rotifera; another tool to die for. Might also want...
by Nikki ONeill
Fri Jun 13, 2014 9:18 pm
Forum: Kiln Casting
Topic: Dental plaster
Replies: 17
Views: 21371

Re: Dental plaster

Great!! info. But please be clear: quatz vs quarts; alumina vs aluminum. Lots of confusion could arise.

Cheers
by Nikki ONeill
Thu Apr 17, 2014 12:20 pm
Forum: Photos and Stuff
Topic: Blankets X 2
Replies: 15
Views: 14978

Re: Blankets X 2

Kudos! Two grey hills design
is especially beautiful.
by Nikki ONeill
Tue Jan 07, 2014 3:05 pm
Forum: Techniques and Tools
Topic: Glue for fused work
Replies: 24
Views: 26419

Re: Glue for fused work

Rave (pump, not aerosol) hairspray works well.

Go to advanced search

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron