Search found 3 matches

by dawirch
Tue Jan 27, 2004 10:07 pm
Forum: Techniques and Tools
Topic: fusing/slumping with a Skutt ceramic kiln
Replies: 10
Views: 17777

fusing/slumping with a Skutt ceramic kiln

I know that this has been talked about a lot on the bulletin board, but I've had trouble finding out if I can definitely use a Skutt ceramic kiln for fusing and slumping, especially the annealing part. I learned fusing/slumping/casting on large glass kilns with Digitry controllers, but alas I no lon...
by dawirch
Mon Jan 26, 2004 1:06 am
Forum: Techniques and Tools
Topic: Dirty glass from Murano - anyone know what it is called?
Replies: 4
Views: 9844

Dirty glass from Murano - anyone know what it is called?

I just got a free box of broken glass from a company that imports blown, colored lamp globes from Italy. All of it has dirt in the glass as if it had been thrown in the batch before it was blown. I was told that this was intentional technique and actually popular among lighting customers. Anyway, I'...
by dawirch
Wed Aug 13, 2003 8:35 pm
Forum: Techniques and Tools
Topic: Has anyone used Ultracal in molds?
Replies: 1
Views: 4762

Has anyone used Ultracal in molds?

Most of the molds I've used for slumping/casting have been a 50/50 plaster/silica mix. I typically get one or two firings before the structure breaks down. I'm trying to find a stronger mold that is not ceramic or steel. I often use Ultracal gypsum cement for non-glass, non-heated molds because of i...