Search found 2 matches
- Fri Jun 28, 2024 11:16 am
- Forum: Kiln Casting
- Topic: acid polishing
- Replies: 11
- Views: 317648
Re: acid polishing
There's information in the paper Skornyakov, M. M., "Acid polishing of glass" 1956, document reference 10.1007/BF00667446 on SciHub.
- Tue Apr 30, 2024 2:22 pm
- Forum: Newcomer Forum
- Topic: Keeping glass in contact with mold crystal clear
- Replies: 1
- Views: 891471
Keeping glass in contact with mold crystal clear
Hi all, dean here, product designer/maker totally new to glass forming. I'm slump forming 3/16" float glass over a graphite mold, and I'd like the result to be as clear as the original glass. The glass comes out of the oven though with a hazy, somewhat rough, surface where it was supported by, ...