Search found 1 match

by lpike
Thu Aug 22, 2024 12:15 pm
Forum: Newcomer Forum
Topic: Help with freeze and fuse
Replies: 6
Views: 190643

Help with freeze and fuse

I am a glass fusing instructor and I have a student who is trying to make game pieces using the Freeze and Fuse technique. He has made his own silicon mold and the pieces are made from powder frit that he ordered from the local glass supply store. The pieces are roughly 1 inch wide and about 2.5 inc...