Search found 1 match

by Diana A
Tue Aug 26, 2003 9:01 am
Forum: Techniques and Tools
Topic: Need help hanging glass without frame
Replies: 9
Views: 23145

Need help hanging glass without frame

Just got a job to create 3 20x20" glass panels for a new home and they want it installed "invisibly", i.e., with no visible framing. Never done this before, but I know a lot of you guys must have. Help! And thanks! :roll: