Search found 4 matches

by glassconfusion
Thu Jan 10, 2008 1:14 pm
Forum: Techniques and Tools
Topic: Freeze and fuse
Replies: 2
Views: 8097

Re: Freeze and fuse

I want to thank EVERYONE for the great discussion and help with this. You guys are the GREATEST! One small thing just to relate, I DID go to the old archives and type in Freeze and Fuse more than once (remember, I am blonde) before I asked the question. I have been on this website since before there...
by glassconfusion
Mon Apr 05, 2004 1:27 am
Forum: Techniques and Tools
Topic: Fusing Uroboros 90
Replies: 9
Views: 25558

Fusing Uroboros 90

I have quite a bit of clear uroboros 90 coe scrap glass which i am trying to fire on my kilnshelf to make a new sheet of glass. It is mostly 2-3 inches by 8-11 inches rectangular and i am butting each piece next to each other, firing in my evenheat coffin kiln at 1500 degrees. I held at 1500 after r...
by glassconfusion
Sat Nov 22, 2003 12:52 am
Forum: Techniques and Tools
Topic: Melting Uroboros Clear Glass
Replies: 1
Views: 5034

Melting Uroboros Clear Glass

I have a great deal of Uroboros clear glass (90) that I want to melt one layer deep in my kiln to form a new sheet of glass. I know it will not be perfectly smooth but what is the range of temperatures (knowing each kiln fires differently) to melt the pieces together to hopefully form a new sheet? t...
by glassconfusion
Sun Sep 07, 2003 9:57 pm
Forum: Techniques and Tools
Topic: Mica Powders One More Time
Replies: 6
Views: 13366

Mica Powders One More Time

Hiya Kids, I need some information please...Im just starting out with the mica powders and I have seen many styles in various glass objects. I use BE and would like to mix the powders and spray them on with a small atomizer or mister.....other than the "medium" that comes with the powders ...