Search found 4 matches

by Andrea
Sat Dec 20, 2003 8:59 am
Forum: Techniques and Tools
Topic: How much ridgidizer?
Replies: 3
Views: 7046

How much ridgidizer?

I have been trying to make a few barrette molds using 1/4 inch fiber blanket and the alumina ridgidizer. I painted the ridgidizer on with a brush, both sides, allowed to dry and then burned off the binder. They were somewhat stiff but when I put the barrettes on and tried to slump they broke in the ...
by Andrea
Sat Nov 08, 2003 9:47 am
Forum: Kiln Casting
Topic: Making ridges on a bowl mold
Replies: 2
Views: 6736

Making ridges on a bowl mold

I am trying to make a series of concrentric circles on an existing mold. I want to then slump a bowl over it to get the ridges in the glass. I have tried several things, a paste of kiln wash (crumbled), clay rings (shrunk and cracked) any ideas? Would calcium hydroxate work? I would like to be able ...
by Andrea
Tue Oct 28, 2003 9:11 am
Forum: Techniques and Tools
Topic: Which side of powder wafer to fuse to base?
Replies: 7
Views: 12908

Which side of powder wafer to fuse to base?

I am wondering if the smooth side of the wafer that was against the kiln shelf will lose its powdery appearance if I fuse that side up under a layer of clear? Would I be better off puting the wafer on top going to full fuse then adding a top layer in another firing? Thanks
by Andrea
Sat Sep 13, 2003 2:19 pm
Forum: Techniques and Tools
Topic: slumping and super spray
Replies: 4
Views: 9787

slumping and super spray

I just fused a piece of bullseye and I ended up with a small area of devit. I was wondering if any of you have tried to use super spray on the devit and slump at the same time? Would I be better off coating with super spray and going back to full fuse then slumping in another firing? I did not put a...