paint it on, fire it, and clear cap it.
Dick
Search found 58 matches
- Mon May 05, 2003 9:05 pm
- Forum: Techniques and Tools
- Topic: lettering on food-friendly glass
- Replies: 2
- Views: 4129
- Mon May 05, 2003 8:59 pm
- Forum: Techniques and Tools
- Topic: Remove imperfections on fused piece
- Replies: 3
- Views: 4213
- Mon May 05, 2003 8:55 pm
- Forum: Techniques and Tools
- Topic: Make a tile saw mobile?
- Replies: 6
- Views: 7079
base
Hi Steve. I bought an HTC 1000 universal base from Amazon for my wet belt. It works great. You adjust it when you build it, and it has locking wheels. My tile saw has a stand and wheels on one end. It works fine. You pick up one end, and wheel it. It came from Harbor Freight.
Dick
Dick
- Tue Apr 08, 2003 10:06 pm
- Forum: Techniques and Tools
- Topic: I am having a problem with my air brush
- Replies: 10
- Views: 12510
- Wed Apr 02, 2003 9:29 pm
- Forum: Techniques and Tools
- Topic: Fusing w/BE Thin Irid
- Replies: 4
- Views: 5481
- Wed Apr 02, 2003 7:24 pm
- Forum: Techniques and Tools
- Topic: healing a crack
- Replies: 3
- Views: 5275
healing a crack
It always happens. I have a 10x16 piece that is 3/4" thick. I wanted to trim it up square before cold working. I guess I got too close to the edge. While cutting, a crack appeared and started across the piece. Can I take it to full fuse and heal the crack, and if so, what type of firing schedul...
- Wed Apr 02, 2003 5:12 pm
- Forum: Techniques and Tools
- Topic: hot start
- Replies: 2
- Views: 4634
hot start
I just got a skutt hot start kiln. I was looking for a small kiln for tests, and small pieces. Most were 300-400 for about a 6"-8". This is just over 500, but takes a 13" shelf, and has a controller. Got it in 3 days, no shipping and it works great.
Just thought I would share.
Dick
Just thought I would share.
Dick
- Wed Apr 02, 2003 5:09 pm
- Forum: Techniques and Tools
- Topic: black pyrex
- Replies: 1
- Views: 3701
black pyrex
Hi all. Does anyone know of a source for black pyrex rod in 1/2" and 1"? I want it for feet. I have bought clear from Winship, but they don't know of black.
Dick
Dick
- Sun Mar 23, 2003 10:21 pm
- Forum: Techniques and Tools
- Topic: wok update
- Replies: 5
- Views: 8250
I sandblasted the rust off the glass. I sanded the wok, heated and recoated. Put the bowl back in, and slumped to 1250 to fire polish. No rust, and a nice satin finish. The only problem is that the clear is not totally clear, and the aventurine is a little matte. Actually for this piece it works nic...
- Wed Mar 19, 2003 8:17 pm
- Forum: Techniques and Tools
- Topic: mold additives
- Replies: 6
- Views: 9940
- Wed Mar 19, 2003 8:15 pm
- Forum: Techniques and Tools
- Topic: Glass Artist TV Shows
- Replies: 3
- Views: 7097
- Wed Mar 19, 2003 5:18 pm
- Forum: Techniques and Tools
- Topic: mold additives
- Replies: 6
- Views: 9940
mold additives
Hi all. I have been using a simple plaster, silica mold mix with good results. I have read about additives such as fiberglass mesh for bigger molds, and for more durability. What exactly do you add, and in what quantities. Finally where do you get the stuff? By the way, molds would be used for slump...
- Wed Mar 19, 2003 1:52 pm
- Forum: Techniques and Tools
- Topic: white mineral deposits
- Replies: 10
- Views: 14457
Hi Bert. I have had the same problem. Sometimes CLR works, sometimes the other products mentioned work. I have had to soak items at times. I have used distilled water as well. I'm thinking that the rocks release some minerals over time, or the combination of dust and dirt settling, and running throu...
- Wed Mar 19, 2003 1:47 pm
- Forum: Techniques and Tools
- Topic: Questions about rock inclusions
- Replies: 16
- Views: 26096
shells
Some shells turn to powder, and some remain. Some just a ghost. You can slump, fuse over them on a bed of sand and get some shell design.
Dick
Dick
- Sat Mar 15, 2003 1:11 pm
- Forum: Techniques and Tools
- Topic: wok update
- Replies: 5
- Views: 8250
wok update
Thanks Tony. I think if I understand you, the frosted look disappears, but it is a matte finish. What I want is for the clear to be clear, or transparent. Matte finish is fine. Is that correct?
Dick
Dick
- Sat Mar 15, 2003 11:09 am
- Forum: Techniques and Tools
- Topic: wok update
- Replies: 5
- Views: 8250
wok update
Well, the rust marks will not come off the glass. I redid the wok, and tried a single piece of clear. No marks. Then someone said that maybe the irid down caused the rust to attach. Question now. If I sandblast the rust off, and want to fire polish, can I place it in the wok, and take it to 1250? I ...
- Mon Mar 10, 2003 2:44 pm
- Forum: Techniques and Tools
- Topic: wok trouble
- Replies: 10
- Views: 16250
wok
I did preheat. I used a torch, heated, sprayed and dried. It was totally dry when it went in the kiln.
Dick
Dick
- Mon Mar 10, 2003 1:10 pm
- Forum: Techniques and Tools
- Topic: wok trouble
- Replies: 10
- Views: 16250
wok trouble
Finally tried my new wok. Sandblasted, sprayed with wash. 19" piece of alternating aventurine green, and clear irid. Got a nice even slump, but where the clear contacted the wok, I had rust come through big time. Left big rust marks on the wok, and minor rust on the glass. I assume I need more ...