Rosanna, It was not an epoch, and thanks. You really made me think. I did set a hold, and it did not happen, and the elements did not shut off. I am going to re-read my kiln manual and do a test run. Another question, if some of the pieces had rather large bubbles, and some had smaller ones, can I r...
- Fri Oct 31, 2003 11:18 pm
- Forum: Techniques and Tools
- Topic: fusing with ceramic kilns
- Replies: 34
- Views: 31215
- Tue Oct 14, 2003 3:15 pm
- Forum: Techniques and Tools
- Topic: fusing with ceramic kilns
- Replies: 34
- Views: 31215
Thanks, I have a cone temp chart, but what I am not sure about is how critical that high temp is to the glass. If I set it to 1465, according to System 96 instructions, and it actually goes up to 1500, will there be a problem with the glass. If so, maybe I should set my hi temp to 1400 expecting it ...
- Tue Oct 14, 2003 2:36 pm
- Forum: Techniques and Tools
- Topic: fusing with ceramic kilns
- Replies: 34
- Views: 31215
- Sat Oct 11, 2003 7:24 pm
- Forum: Techniques and Tools
- Topic: fusing with ceramic kilns
- Replies: 34
- Views: 31215
Thanks for your replys. The kiln is going. I set a ramp hold program following Spectrums recommended schedule. The high temp was 1465, and the kiln shut off on schedule, but the temp kept rising, so I opened it a crack to flash vent down to 1000. Then, the temp started rising again, so I stopped the...
- Fri Oct 10, 2003 10:58 pm
- Forum: Techniques and Tools
- Topic: fusing with ceramic kilns
- Replies: 34
- Views: 31215
Automatic ceramic kiln
I am about to start my first fusing project in my Skutt automatic ceramic kiln. I've read all of the posts here, but am still confused. I still have a few specific questions: 1. I have an automatic kiln, so can just fire to cone 016m or program it to follow the System96 standard firing schedule? 2. ...