Kiln wash

I am firing Spectrum together to fuse completely - two pieces, bringing the temp to 1415 degrees. I have several small pieces in the kiln on a newly kiln washed surface, sprayed several layers & dry. Almost all the pieces have kiln wash stuck to them, except two which are larger than the others ...