Search found 5 matches
- Sat Feb 28, 2004 11:02 am
- Forum: Techniques and Tools
- Topic: Jen-Ken vs. Skutt vs. Paragon
- Replies: 9
- Views: 25972
I recently purchased a Paragon GL-24AD and have mixed feelings. The kiln is awesome. The only thing I wish was that the peek holes were in a better location. (It's very difficult to see inside, without opening the door.) The service from Paragon was terrible. I waited over 5 weeks for my kiln, when ...
- Sun Jan 18, 2004 11:14 am
- Forum: Techniques and Tools
- Topic: Has anyone used new Spectrum S96 "high fire" irids
- Replies: 2
- Views: 6759
http://community.webshots.com/photo/112 ... 5523GMYbWG
I've been using the black Hi-Fire and I'm very happy with it! On the picture you can see what it looks like capped and not capped. I've got the clear also, but I have not experimented with it yet.
I've been using the black Hi-Fire and I'm very happy with it! On the picture you can see what it looks like capped and not capped. I've got the clear also, but I have not experimented with it yet.
- Tue Jan 06, 2004 8:24 pm
- Forum: Photos and Stuff
- Topic: What did I do? Fusing gone bad!
- Replies: 10
- Views: 16916
- Tue Jan 06, 2004 9:26 am
- Forum: Photos and Stuff
- Topic: What did I do? Fusing gone bad!
- Replies: 10
- Views: 16916
Thanks for all of your help! It wasn't refired. That is the original fire. I did cap it with clear. The clear is BE compatible. the light blue is Uroboros that was not listed as compatible, but I did a test strip and it turned out okay. The streaky blue was an unknown glass that I had and again test...
- Mon Jan 05, 2004 11:46 pm
- Forum: Photos and Stuff
- Topic: What did I do? Fusing gone bad!
- Replies: 10
- Views: 16916
What did I do? Fusing gone bad!
I'm new to fusing and I'd like your opinion as to what I did wrong. I did a test strip with all of the glass and it looked like it was all compatible. I suspect that I'm reading my stressometer incorrectly. Can you tell by the break pattern? Thanks for your help! Deb http://community.webshots.com/ph...