- Fri Aug 03, 2012 6:25 pm
- Forum: Techniques and Tools
- Topic: firing detail on a plate with interior rim
- Replies: 1
- Views: 3805
firing detail on a plate with interior rim
I'm firing Spectrum 96 (clear base with multi pieced top layer. The mold has an interior 1/2" rim that I want to line with diachroic chips. I'm thinking if I fire the chips in the first full fuse firing, I could mis-align (since the late has a shallow dip to it). If the chips are small enough w...
- Mon Dec 08, 2003 8:50 pm
- Forum: Techniques and Tools
- Topic: Avoiding bubbles when fusing
- Replies: 2
- Views: 5114
Avoiding bubbles when fusing
:roll: I'm using Spectrum 96 glass, two layers or 1/4" plus small detail in an overall 14" diameter round. I understand to avoid bubbles, it helps to do a "ramp freeze" so I went 60 dpr to 1300 then 4000 dph to 1480, then 1200 dph to 1000, 300 to 955555 and finally 200 to 800 and...