Search found 2 matches

by unicorn
Mon Jul 08, 2013 7:35 pm
Forum: Techniques and Tools
Topic: Iridised glass which way up
Replies: 9
Views: 18900

Re: Iridised glass which way up

Hi Paul
We spoke on the phone some years back, I just came across your business card and wondered how it was going for you and how you fared after the earthquakes?
I tried your website: www.paulschulz.co.nz but it doesn't appear to work.
Cheers
Jon
jon@unicornglass.com
by unicorn
Fri Dec 19, 2003 8:31 pm
Forum: Techniques and Tools
Topic: float/slump/devit?
Replies: 5
Views: 8180

Hi Ya. It would really help to know which was the metal side of the float. If you fire metal side up there is a good chance you'll get de vit. An ultraviolet lamp can be used to determin which is the metal side, but an old glazier told me he could taste the metal by licking the glass, yuk.