Search found 287 matches
- Wed Aug 13, 2003 1:18 am
- Forum: Business Topics
- Topic: Ouch! Does smart business=evil artist?
- Replies: 92
- Views: 92208
First, the more people who see kiln carved architectural glass and glass sinks, the more people there will be who are thinking that they want some for themselves. My work will speak for itself and I'll get more business. --snip-- I respect Bob's approach of teaching a basic technique but not teachi...
- Wed Aug 13, 2003 12:11 am
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
- Mon Aug 11, 2003 6:32 pm
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
- Mon Aug 11, 2003 2:29 pm
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
Go back a couple of weeks and read the thread on gold leaf and micas http://www.warmglass.com/phpBB/viewtopic.php?t=1772. I think you'll find that there are a number of people who have experienced this phenomenon with a number of different glasses. Ted Sawyer may be a good person to ask... but don'...
- Mon Aug 11, 2003 1:12 pm
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
This sounds similar to the irid down problem that I've seen in the past, bust always with a black base glass... you can cratch the irid off with a fingernail and it's pitted under the surface. no answers... just validation Tony Hi Tony... YES. Do you think it's actually devit? Anyway, your descript...
- Mon Aug 11, 2003 12:11 pm
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
PS
P.S. your other questions, Bob....
Is the irid surface pitted?
YES.
Do granules of glass pop out?
No. Some of the crystals seem raised, tho.
Muchos gracias again, Bob.
xxoo
BB
Is the irid surface pitted?
YES.
Do granules of glass pop out?
No. Some of the crystals seem raised, tho.
Muchos gracias again, Bob.
xxoo
BB
- Mon Aug 11, 2003 11:58 am
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
- Sun Aug 10, 2003 6:37 pm
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
I'll try plopping the problem area on the scanner ... if it works, you'll see what I mean. Here are 2 scans. There are more at http://www.pbase.com/pdxbarbara/crystalized_irid_mystery_pix if ya'll get excited about this problem... Thanks guys... BB In the 2nd pic, the irid scratched off when I trie...
- Sun Aug 10, 2003 1:30 pm
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
Barbara, does the location and shape of the problem area have any relation to the size and shape of anything slumped on this mold in the past? Different glasses seem to affect kilnwash differently. Some seem to leave more flux in the kilnwash than others as seen by the discoloration of the kilnwash...
- Sun Aug 10, 2003 12:58 pm
- Forum: Photos and Stuff
- Topic: BECon pix
- Replies: 15
- Views: 17459
- Sun Aug 10, 2003 3:51 am
- Forum: Photos and Stuff
- Topic: BECon pix
- Replies: 15
- Views: 17459
- Sun Aug 10, 2003 3:48 am
- Forum: Photos and Stuff
- Topic: BECon pix
- Replies: 15
- Views: 17459
- Sun Aug 10, 2003 3:37 am
- Forum: Techniques and Tools
- Topic: Crystal irid
- Replies: 18
- Views: 13310
Crystal irid
Got some crystalization on irid. Slumping on kilnwashed (BE wash) SS plate. BE 1116 (turquoise blue) irid down tried to scrub it off (scotchbrite kinda thing, gently w/ wire brush. Actually took off some of the irid. Never seen this before. Usually the irid down helps with the release. Plus the crys...
- Sat Aug 09, 2003 2:23 pm
- Forum: Photos and Stuff
- Topic: New Series
- Replies: 5
- Views: 7955
Re: New Series
Both are lovely, but I'm partial to the Mariposa series. Like clover leaf windows on universal cosmic phenomena...afilloon wrote:
Dinah and I have begun working on a couple of new series and would like your thoughts.
Thanks for showing.
Barbara
- Sat Aug 09, 2003 3:19 am
- Forum: Photos and Stuff
- Topic: Jackie's piece...
- Replies: 21
- Views: 23177
- Sat Aug 09, 2003 2:57 am
- Forum: Photos and Stuff
- Topic: BECon pix
- Replies: 15
- Views: 17459
BECon pix
Go to http://www.pbase.com/pdxbarbara/whats_new & click on BECon. Sorry some pix suck, and tired of uploading for now anyways..... The glass is from the Legacy exhibit. All pairs are the teacher/student matches. Don't have 'm all here. Barbara Here's Nancy Weisser's contribution... http://www.pb...
- Sat Aug 09, 2003 2:52 am
- Forum: Photos and Stuff
- Topic: Jackie's piece...
- Replies: 21
- Views: 23177
- Fri Aug 08, 2003 2:28 pm
- Forum: Photos and Stuff
- Topic: Jackie's piece...
- Replies: 21
- Views: 23177
YAAAAAY for me....
I did it...Hey Paul & Bert... lookee here! I got a photo posted...
Thanks for the help.
BB
Thanks for the help.
BB
- Fri Aug 08, 2003 2:25 pm
- Forum: Photos and Stuff
- Topic: Jackie's piece...
- Replies: 21
- Views: 23177
Re: Jackie's piece...
HERE I GO...PDXBarbara (Bader) wrote:hang on... trying to post pix for 1st time...
![Image](http://www.pbase.com/image/20136141.jpg)
- Fri Aug 08, 2003 12:38 pm
- Forum: Photos and Stuff
- Topic: Jackie's piece...
- Replies: 21
- Views: 23177