stainless floral former
I just bought a cple of new stainless floral former and Hitemp1800
Sprayed them, fired them to 700.
Put glass on when cold, set in kiln with some that I have had for years, the glass on new former stuck and broke, older ones were fine.
Any ideas?
tks
Sprayed them, fired them to 700.
Put glass on when cold, set in kiln with some that I have had for years, the glass on new former stuck and broke, older ones were fine.
Any ideas?
tks
- Fri Apr 09, 2004 12:28 pm
- Forum: Techniques and Tools
- Topic: first time using ceramic molds
- Replies: 7
- Views: 19582
first time using ceramic molds
Having never used a ceramic mold, a couple questions: 3 or 4 coats of kiln wash? prefire to ?? how long before needing to kiln wash again do you sand off when needed or can you actually rinse of kiln wash with water? will most glass slump at app 1200 - 1250? one more question, how the heck do you va...
- Tue Mar 09, 2004 1:45 pm
- Forum: Techniques and Tools
- Topic: bisque/float glass question
- Replies: 1
- Views: 4251
bisque/float glass question
Morning from BC Can I get opinion(s) on the following 12" square of float over a treated bisque form and used the following firing sche in my skutt: 370' ph to 1100 9999' ph to 1325 soak for 14mins ( was fine at this point , that I could see) 9999' ph to 950 150'ph to 750 500' ph to 0000 when I...
- Thu Feb 26, 2004 10:21 pm
- Forum: Techniques and Tools
- Topic: bisque
- Replies: 1
- Views: 4694
bisque
Can anyone give me some info on using bisque forms, how many layers of kiln wash, do I refire after spraying with kiln wash before adding glass, can I slump over it or only on the inside, thanks, Archie
- Thu Feb 19, 2004 4:24 pm
- Forum: Techniques and Tools
- Topic: newbie float question
- Replies: 13
- Views: 29471
newbie float question
afternoon
If I wanted to try a bowl, ect using float glass and I should use 2 layers of glass? can I cap colored float with clear or should I use two layers of the colored? Can anyone give me a suggestion for a firing sched for a Skutt? thanks, Archie
If I wanted to try a bowl, ect using float glass and I should use 2 layers of glass? can I cap colored float with clear or should I use two layers of the colored? Can anyone give me a suggestion for a firing sched for a Skutt? thanks, Archie
- Tue Feb 17, 2004 11:08 am
- Forum: Techniques and Tools
- Topic: float glass
- Replies: 2
- Views: 5619
float glass
thanks, I will give it a try, archie
- Mon Feb 16, 2004 11:47 pm
- Forum: Techniques and Tools
- Topic: float glass
- Replies: 2
- Views: 5619
float glass
evening, I would like to try making a bowl, app 12 - 14" across , out of float glass, Is there a schedule somewhere for float, I'm not having much luck finding one. Does anyone know if the preprogramed scheds that come with the "Skutt GM814" are for float? Would I fuse together at lea...
- Tue Feb 03, 2004 4:23 pm
- Forum: Techniques and Tools
- Topic: fusing/slumping question
- Replies: 2
- Views: 5881
s/s form
thanks for the info, archie
- Mon Feb 02, 2004 12:19 pm
- Forum: Techniques and Tools
- Topic: fusing/slumping question
- Replies: 2
- Views: 5881
fusing/slumping question
morning from Vancouver Isl I have a couple of questions, any suggestions would be appr. I have just fused my first pieces of glass together to later slump into a bowl-2 pieces of 9" circle, bottom slightly smaller with some smaller pieces on top of both for pattern 1. do most people heat the st...
- Mon Jan 26, 2004 5:30 pm
- Forum: Techniques and Tools
- Topic: first firing
- Replies: 2
- Views: 5504
- Mon Jan 26, 2004 3:32 pm
- Forum: Techniques and Tools
- Topic: first firing
- Replies: 2
- Views: 5504
first firing
morning from BC, I tried my first firing yesterday, following the book I did coasters first, the two that I did exactly as the book suggested turned out fine though the edges were a little rough, another I put a 2" square of aluminun foil between layers and it had a couple bubbles that made it ...
- Mon Jan 26, 2004 1:27 pm
- Forum: Techniques and Tools
- Topic: new to kiln
- Replies: 15
- Views: 23105
- Sat Jan 24, 2004 2:07 pm
- Forum: Techniques and Tools
- Topic: new to kiln
- Replies: 15
- Views: 23105
- Sat Jan 24, 2004 1:56 pm
- Forum: Techniques and Tools
- Topic: new to kiln
- Replies: 15
- Views: 23105
new to kiln
morning, hope this isn't coming up twice My husband bought me a Skutt814 for Christmas, I haven't tried it out yet, just got wired yesterday, thought I would practice with coasters but wandered if anyone has ever done wine/beer bottles on their side, thanks for any suggestions and I have learnt lots...