I took it to 1700, then i combed, then held at 1700 for 30 min. I was a
little afraid that i would comb too hard and go thru glass into shelf.

John
by joeat
Tue Mar 09, 2004 11:56 pm
Forum: Photos and Stuff
Topic: First Combing Try
Replies: 2
Views: 6675

First Combing Try

My first attempt at combing, i probably didn't move tool around enough, but as i said it's my first attempt. Let me know what you think. The help that i get here makes me want to try new things, and i know that i will only get good advice. Thanks John http://community.webshots.com/photo/124350231/12...
by joeat
Sun Mar 07, 2004 12:57 am
Forum: Photos and Stuff
Topic: Had to try Potmelt
Replies: 8
Views: 15153

Thanks Jon for the comment as for the hole size it was around 1 inch
trying to make it as round as possible and i cut 8 slots of about 1/16th inch that radiated outward. Don't know if that made any difference or not.

John
by joeat
Sun Mar 07, 2004 12:43 am
Forum: Photos and Stuff
Topic: Had to try Potmelt
Replies: 8
Views: 15153

Thanks for the comments on my potmelts, as of now i don't have any
plan for their use. They were on the small size from 2 inch to 4 inch.with
a thickness close to 1/4th inch. And the pots were around 4.5 inch big.
Will try and make a larger one with only 2 colors to see how it turns out.

John
by joeat
Fri Mar 05, 2004 10:00 pm
Forum: Photos and Stuff
Topic: Had to try Potmelt
Replies: 8
Views: 15153

Had to try Potmelt

After reading and seeing the results of others I too had to try my hand at Potmelts. Don't know if i used too many colors, because they seem too (for the lack of a better word) busy. Had no trouble with the process and left over glass stuck to pot (39 cents at Michaels). When loading should i random...
by joeat
Sun Feb 08, 2004 8:27 pm
Forum: Techniques and Tools
Topic: what happened to my dollar bill
Replies: 4
Views: 9328

Thanks for the help. I fired to a temp of 1485, i may try raising the top piece at the corners so the air will escape, i read that it allows the air, gas to escape before it fully fuses.
john
by joeat
Sat Feb 07, 2004 10:21 pm
Forum: Techniques and Tools
Topic: what happened to my dollar bill
Replies: 4
Views: 9328

what happened to my dollar bill

Tried the dollar bill between to clear pieces. Came out with big air bubble
a little negative image on back side but that's all. Thought it would look
better that this. Or is this what i am to expect? http://community.webshots.com/photo/116 ... 1706Ykzvsm
Help appreciated.
John
by joeat
Sun Jan 18, 2004 3:06 pm
Forum: Photos and Stuff
Topic: Comments on picture frame
Replies: 6
Views: 10838

by joeat
Sun Jan 18, 2004 1:32 pm
Forum: Photos and Stuff
Topic: Comments on picture frame
Replies: 6
Views: 10838

sorry bout that didn't check one of the options, hopefully it will work now
by joeat
Sun Jan 18, 2004 12:30 pm
Forum: Photos and Stuff
Topic: Comments on picture frame
Replies: 6
Views: 10838

Comments on picture frame

New to fusing, am making picture frames for my 3 sons graduation pictures.This is the first one and it came out ok except for hazy look on 2/3rds of clear cap glass. Probably due to cleaning. But am learing so hope i won't make same mistake again. http://community.webshots.com/s/image9/9/15/61/11209...
by joeat
Sun Jan 18, 2004 12:18 am
Forum: Techniques and Tools
Topic: Hazy look after clear cap
Replies: 1
Views: 4029

Hazy look after clear cap

This is my first attempt at fusing, have read books and have been checking out the Bulletin Board Forums. Made a picture frame using Sys 96 glass, it came out ok for my first try. But i thought it would look better capped with clear glass. Fused piece again but about 2/3rds of it came out hazy, the ...