Search found 2 matches

by katfaerie
Tue Jan 27, 2004 9:42 am
Forum: Techniques and Tools
Topic: fused glass jewelry questions
Replies: 9
Views: 18239

thanks for the info so far. :D the kilns that i am currently looking at include the paragon caldera from bullseye and a jen-ken with infinity controller and built in pyrometer. anybody use either? does the infinity controller more or less work like a digital temp controller? any more info would be g...
by katfaerie
Mon Jan 26, 2004 10:16 pm
Forum: Techniques and Tools
Topic: fused glass jewelry questions
Replies: 9
Views: 18239

fused glass jewelry questions

hi, i'm just about to purchase my very first kiln. i am interested in making small fused glass pieces, pendants, and beads mostly. i have taken a fused glass class, but did not get to fire anything. i need to know specifics on how to fire my pieces (how long?), and really what kind of kiln to buy. d...