Search found 11 matches
- Fri Feb 06, 2004 2:34 pm
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
Tony, Thanks for the info and continued support!! I just noticed that you are from Ithaca. Are you connected with Corning Museum?? I love that place and hope to take some classes there in the future. I've never been to a more interesting museum, not just because I love glass either......my family hu...
- Fri Feb 06, 2004 10:33 am
- Forum: Techniques and Tools
- Topic: Kiln Evenivity
- Replies: 6
- Views: 13584
- Fri Feb 06, 2004 10:27 am
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
O.K. I am not quite ready to do a happy dance, but I am getting close. Heres what I have discovered and what the final results are. My shelves are flat. My kiln is firing hotter than it thinks!! my firing schedule yesterday was incredibly conservative: 250 dph to 980 soak for 20 60 dph to 1285 soak ...
- Thu Feb 05, 2004 4:39 pm
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
Deborah, I dont know that I can offer much more than a shoulder to cry on. I am really trying to slow down the whole firing process. I am actually ramping 250 to 980, holding for 20 than 60 to 1285 holding for 20 than 250 to 1435. I am trying this with bullseye. I have discovered that this new kiln ...
- Thu Feb 05, 2004 12:28 pm
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
Tony Thanks for the info. I am currently firing my kiln. I am using a much slower ramp time. Yes I am finding that this larger kiln seems to hold a temp and fuses at a lower range than my smaller one. I really think that the size of the shelve has alot to do with it, as I am using two large shelves,...
- Wed Feb 04, 2004 10:08 pm
- Forum: Photos and Stuff
- Topic: A little splash of color
- Replies: 30
- Views: 53128
- Wed Feb 04, 2004 10:02 pm
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
Ron, Thanks for the good info. I didnt get around to firing today, however am ready to go for tomorrow. I got very similar advice today from a good friend. She stated about the same as you, that I need to slow down, and that my glass is starting to lay flat around the edges but remainin cooler in th...
- Tue Feb 03, 2004 6:36 pm
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
OK tommorrow will be a new test fire with my old shelve. I think I will also make one with fiber board and try that. SSSHHHEEEESSSHH Thanks for your quick input. You know how it goes......I am not sleeping at night because my brain loves a good mystery!!!! I just dont like loosing all of the glass.....
- Tue Feb 03, 2004 5:49 pm
- Forum: Techniques and Tools
- Topic: Fiber Board from Warm Glass
- Replies: 6
- Views: 12118
- Tue Feb 03, 2004 5:47 pm
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
Bubbles and evenheat kiln
Thanks for the quick reply. I have placed a level on my shelves and they appear to be flat. I am assuming that is an accuate test.????
- Tue Feb 03, 2004 4:46 pm
- Forum: Techniques and Tools
- Topic: have new evenheat GTS 2541 and am experiencing BIG BUBBLES
- Replies: 18
- Views: 42605
have new evenheat GTS 2541 and am experiencing BIG BUBBLES
I have just started using my new evenheat GTS 2541-13. I have been fusing glass for three years with smaller kilns and never had such a problem I am having now. I have been doing test fires with Spectrum 96 and Bullseye 90 and am experiencing the same problem......you guessed it !!! Huge Big Blister...