Search found 1 match

by Guy_o
Thu Feb 12, 2004 4:52 pm
Forum: Techniques and Tools
Topic: Bubbles Problems in Fusion
Replies: 1
Views: 4930

Bubbles Problems in Fusion

I tried to fuse 3 pieces of float glass 24x24 inch wide and 1/4 inch thick without any bubbles.
I did many test but the result is not perfect.

So, if anybody can help me I would apreciate.

Thanks
Guyo