Search found 4 matches

by Linda Huffman
Thu Jul 10, 2003 3:19 pm
Forum: Techniques and Tools
Topic: confused about adhesive for mirror
Replies: 12
Views: 54994

For those of you who are interested in what the mfg. had to say, here's the email I received from them this morning. (I asked permission from them to post it here and they agreed.): "Thanks for writing and letting us know what your hearing out in the retail market. However, the product has not ...
by Linda Huffman
Wed Jul 09, 2003 10:16 pm
Forum: Techniques and Tools
Topic: confused about adhesive for mirror
Replies: 12
Views: 54994

Barbara, that's very interesting. I just checked their (Liquid Nails) web site and it also claims that it doesn't desilver mirror. I sent an email to the mfg. and will post their reply when it comes in.
by Linda Huffman
Wed Jul 09, 2003 12:19 pm
Forum: Techniques and Tools
Topic: confused about adhesive for mirror
Replies: 12
Views: 54994

I recently purchased some "Liquid Nails" adhesive that's made just for use with mirrors. The writing on the tube says that it "......will not desilver electro-copper plated mirrors."
by Linda Huffman
Wed Jul 09, 2003 12:13 pm
Forum: Techniques and Tools
Topic: jewelry findings for fused glass jewelry?
Replies: 13
Views: 33398

Check out "Rings & Things", http://www.rings-things.com and the phone # is 1-800-366-2156. They have inexpensive "glue-on drop loops" that you glue your cab onto. (It has a loop for a jump ring to attach to your chain or cord.) I just looked in my most recent catalog and the ...