Re: CHANGE OF COLOR
Brian, Thanks for the advise. I am ashamed and embarassed to admit I do not know what is tungsten carbide [sounds like strange medicine to me :? ] sorry for appearing so stupid. They say in our tradition that the shy person will not learn............ Havi Hard metal Close 2 diomond in hardness use ...
- Mon Dec 17, 2007 12:11 pm
- Forum: Newcomer Forum
- Topic: CHANGE OF COLOR
- Replies: 3
- Views: 13455
Re: CHANGE OF COLOR
Thanks Gundi, Unfortunately, I can not see any difference between BE 1101 and or BE 1824, and/or 1831 - even if you look at them from the side. Others I can see . thanx anyway Havi Havi Try a long sample assembly Make a pieces of known glass say 30 mm x 100 mm longer is better mark with letter tung...
- Tue Apr 13, 2004 6:02 am
- Forum: Business Topics
- Topic: "Collectors' Discount"
- Replies: 30
- Views: 84495
Re: "Collectors' Discount"
I just started coming up against this recently: at retail shows buyers are asking for The Discount, not just "can you do any better?" but "can I have a collectors' discount ? First they tell me about their Chihuly, their Moje, their John Kuhn, and then we discuss the work in front of...
- Mon Apr 12, 2004 6:10 am
- Forum: Techniques and Tools
- Topic: any experienced deviter lobbying with a spare minut read me
- Replies: 5
- Views: 13644
Re: any experienced deviter lobbying with a spare minut read
I've been asked to make some 4' and 2 inch square tiles for a washroom from tempered chunks devitrified. I have come to the conclusion that the amount of devit I get may depend where the float came from. -Does a "cloudier" tinside mean your going to have more/less devit ? -Can anyone tell...
- Wed Mar 31, 2004 4:50 am
- Forum: Techniques and Tools
- Topic: breakthrough rigidizer news
- Replies: 38
- Views: 55184
- Thu Mar 25, 2004 7:03 am
- Forum: Techniques and Tools
- Topic: Lessons Learned . . .
- Replies: 25
- Views: 43988
Re: Lessons Learned . . .
the hard way! Lesson #1: When two of the relays in your kiln fail, replace them all. Why: I recently replaced two of the four relays in my Paragon GL24AD kiln. A couple of firings later, yup, another one failed. Two more are now on order. Lesson #2: When you're having relay problems, DON'T USE THE ...
- Thu Mar 18, 2004 6:26 am
- Forum: Techniques and Tools
- Topic: How do you see new work
- Replies: 22
- Views: 46188
Re: How do you see new work
Ok, I've been hanging out here this afternoon. I was reading the thread that Jackie started and then took a long look at the photographer's web site that Lani posted. The images on the photographer's site got me thinking, how did they envision these images. Then I thought about how I envision my wo...
- Thu Mar 18, 2004 5:31 am
- Forum: Techniques and Tools
- Topic: Warm Glass Dictionary
- Replies: 43
- Views: 72979
Re: Warm Glass Dictionary
Thanks to Lauri Levanto, we have a preliminary draft of an online dictionary of kiln-forming terms. Please check it out and let us know what you think. This is a draft, not a final version, so comments are encouraged. If you have suggestions for improvement, terms to add, or corrections, please not...
- Wed Mar 17, 2004 6:10 am
- Forum: Techniques and Tools
- Topic: Warm Glass Dictionary
- Replies: 43
- Views: 72979
Re: Warm Glass Dictionary
Thanks to Lauri Levanto, we have a preliminary draft of an online dictionary of kiln-forming terms. Please check it out and let us know what you think. This is a draft, not a final version, so comments are encouraged. If you have suggestions for improvement, terms to add, or corrections, please not...
- Mon Mar 15, 2004 7:26 am
- Forum: Techniques and Tools
- Topic: breakthrough rigidizer news
- Replies: 38
- Views: 55184
Re: breakthrough rigidizer news
Explain which bit ???Stuart Clayman wrote:Brian,Brian and Jenny Blanthorn wrote: .Bat Wash
Brian
I know I can be a little Batty at times, and I do like to get washed but I don't think that is what you were referring to as Bat Wash.. can you explain?
Brian
- Mon Mar 15, 2004 7:18 am
- Forum: Techniques and Tools
- Topic: Reconciling Temp Differences Between Kilns
- Replies: 19
- Views: 31094
Re: Reconciling Temp Differences Between Kilns
Hi. After 9 years with a Paragon GL22AD, I just added a Skutt Clamshell to my armamentarium. Both great kilns, but I'm finding that the Skutt fires at different temps than my Paragon. It seems that I achieve the same effects in the Skutt at temps about 40 degrees lower than the Paragon. eg an "...
- Fri Mar 12, 2004 6:00 am
- Forum: Techniques and Tools
- Topic: Pigment of my imagination?
- Replies: 34
- Views: 49461
that's what he implied, but didn't state. i would suppose that the chemicals used would migrate or otherwise change in some manner at fusing temps though, so they still might go away. i suspect a very low slump temp of uro in a single layer might work. you might still get devit though, and low temp...
- Fri Mar 12, 2004 5:37 am
- Forum: Techniques and Tools
- Topic: breakthrough rigidizer news
- Replies: 38
- Views: 55184
Re: breakthrough rigidizer news
.[/url][/quote] Yo Bert Sounds good But I thought a colliod was some stuff u only got as as solution As far as I know u cant get collidal silica as a powder There was some about using colloidal alumina as part of a glass furnace construction over craftweb Does colloidal alumina separate out after mi...
- Fri Mar 12, 2004 5:23 am
- Forum: Techniques and Tools
- Topic: breakthrough rigidizer news
- Replies: 38
- Views: 55184
Re: breakthrough rigidizer news
I just spoke to Wes Jones at Wesbond corp. They are a maker of rigidizers that major companies buy from. They make both colloidal silica and alumina. He told me that colloidal alumina seems like a much better material to be rigidizing boards with, for several reasons. The silica turns to crystaboli...
- Thu Mar 11, 2004 9:42 am
- Forum: Techniques and Tools
- Topic: Pigment of my imagination?
- Replies: 34
- Views: 49461
Re: Pigment of my imagination?
i'm always curious why there isn't a good magenta or fuschia in the color lines of any of the fusible, and why the most intriguing ring mottles don't handle fusing well - no i've not tried them but i've been told they don't like going to full fuse but i would love to fuse a layer of ring mottles to...
- Thu Mar 11, 2004 9:36 am
- Forum: Techniques and Tools
- Topic: Pigment of my imagination?
- Replies: 34
- Views: 49461
Re: Pigment of my imagination?
I've been watching colors develop in Bullseye glass and I'm trying to understand the reason. I'm familiar with the process of "striking" for red and orange opal glass and see the results often. Is it the same process when other colors seem to develop after firing a time or two? Example, s...
- Thu Mar 11, 2004 9:28 am
- Forum: Techniques and Tools
- Topic: Pigment of my imagination?
- Replies: 34
- Views: 49461
- Mon Mar 08, 2004 12:00 pm
- Forum: Techniques and Tools
- Topic: Rollin' & Tumblin'
- Replies: 18
- Views: 30986
Re: Rockin & Tumblin
Here are a couple links you might find useful. http://www.gemworld.com/Tumbling.asp http://www.memphisgeology.org/tips_tumbling.html While the material may be different- the procedure remains the same. Steve Gem world is a good link But glass is a lot more difficult due 2 fractures In adition 2 the...
- Mon Mar 08, 2004 11:46 am
- Forum: Techniques and Tools
- Topic: Rollin' & Tumblin'
- Replies: 18
- Views: 30986
- Mon Mar 08, 2004 7:18 am
- Forum: Techniques and Tools
- Topic: Rollin' & Tumblin'
- Replies: 18
- Views: 30986
Brian wrote: Use liquidised news paper / paper kittly litter Pasty sludge sounds Ok Watch out 4 gassing a tiny drop of bleach may help You are recycling ? Does it gas out if I apply unused kitty litter -lauri :shock: I'm confused. The bleach is added to the pasty sludge in the kitty litter? Do we d...