firing surface

just curious, how many fire fused glass projects on 1/8th inch fiber paper or directly on a kiln- washed shelf are there advantages , disadvantages? I've noticed the pieces fused on fiber paper are generally cleaner and cool better. just wondering what y'all find better. thanks