wire for wine bottle fuse

Just a quick question regarding the hangers for slumped wine bottles, how is it possible to attach a wire to hang the finished product, I've tried glue, doesn't hold, :?: even fusing a piece of wire into the glass, but it cracks, any suggestions? thanks
by Terrik
Wed Mar 31, 2004 4:18 pm
Forum: Techniques and Tools
Topic: pot melting
Replies: 1
Views: 3938

pot melting

I'm confused. I'm attempting a pot melt of my scrap glass. If I fill a pot with glass and suspend it 4" or so from my saucer, what do I suspend it with, if I use kiln posts they obviously will end up fused to the glass, even if I melt onto my shelf, the post will end up in the glass? I guess I'...