Re: Drilling holes in Molds
It may just be that there are copper inclusions. I purchased a flat panel which has copper inclusions. It is two layers of glass thick with the copper in between. The top of the panel dips down into the "empty holes" of the copper pattern and down again around the edges of the inclusions. ...
- Mon Jun 18, 2012 12:38 pm
- Forum: Techniques and Tools
- Topic: Schedule taking too long
- Replies: 17
- Views: 38514
Re: Schedule taking too long
I see that kind of problem when my relay needs replacing.
The controller also starts giving messages about low firing rates.
The controller also starts giving messages about low firing rates.
- Sat Apr 17, 2004 9:43 am
- Forum: Techniques and Tools
- Topic: This was buried in another post so not many people saw it...
- Replies: 6
- Views: 20732
- Sun Apr 11, 2004 9:58 am
- Forum: Techniques and Tools
- Topic: Amended Challenge
- Replies: 88
- Views: 2952133
:shock: I too would like to try this challenge :shock: I am so new to warm glass I am not sure I have a style yet. But black and white, and a realistic subject would be opposite of my usuall style So... it looks like I would need to be up dated on standard proceedures here. When is the due date? Sus...
- Thu Apr 08, 2004 11:07 am
- Forum: Techniques and Tools
- Topic: kiln shelf bubbles
- Replies: 12
- Views: 28017
kiln shelf bubbles
I am new to fusing. The last three pieces I have done, about 8x10 inches, have all had a rather large, rather annoying bubble in them. This is a bubble from under the bottom layer of glass. After doing the second piece, it crossed my mind that the bubble might be due to the kiln shelf itself. So the...
- Thu Apr 08, 2004 10:58 am
- Forum: Techniques and Tools
- Topic: would like to hear everyones opinion about sandblast setup
- Replies: 9
- Views: 19907
I have one I stand at, My son bought it for me, so I have no idea of the make. I stand on several paving stones to make the arm holes the correct height for me. Or if you are tall, put the cabinet on blocks to make it the correct height for you. I mostly like the pass through feature the cabinet has...