Search found 2 matches
- Fri Apr 02, 2004 3:27 pm
- Forum: Kiln Casting
- Topic: Cobalt Bottles for Casting ?
- Replies: 14
- Views: 30097
hi Bert. my question is a bit off topic. i use a dry 50/50 mix of gypsum plaster and silica sand for float glass slumping. will this dry mix still be happy above 1400 F? thank you nelson It will be happy enough but it won't soak up water and harden into a mold after you fire it. There is some water...
- Wed Mar 31, 2004 3:15 pm
- Forum: Kiln Casting
- Topic: Box Casting.Has anyone experienced devit?
- Replies: 22
- Views: 50891
Splash Coat?
I have just begun casting. Have completed one piece with about 4 lbs. glass and 1 in. thick. I used the 50/50 plaster/silica mix. the piece came out pretty good. Since it was a test I used float. Now to the question...What is a 'spash coat'. Please explain and tell how to to do it .
Thanks
TH
Thanks
TH