Search found 3 matches

by eclairewl
Tue Apr 15, 2014 7:17 am
Forum: Jewelry Making
Topic: domed pendant
Replies: 4
Views: 144387

Re: domed pendant

It was definitely fused but I think I finally figured out how it was done: by heating the 2 pieces to 1500 I was able to achieve the effect.
Thanks for your help.
by eclairewl
Mon Apr 14, 2014 10:33 am
Forum: Jewelry Making
Topic: domed pendant
Replies: 4
Views: 144387

Re: domed pendant

These are 1 inch circles with a convex suface. I am going to give it a try making my round pendant flat and using a slightly larger piece of glass over it. I do this for small earrings but haven't tried it for larger pieces.
by eclairewl
Sun Apr 13, 2014 3:14 pm
Forum: Jewelry Making
Topic: domed pendant
Replies: 4
Views: 144387

domed pendant

I bought a pendant in Spain that was a domed circle and I have been trying to figure out how to do this.
Any ideas?