Re: How can we make dichroic nametags?
for the decal "paper" you can use any Contact paper, like they used to line drawers with. Clear is the easiest to work with, the idea is that you should be able to cut or paper punch it and it should stick during the etching process. It's a fun technique, have fun with it.
- Sat Dec 15, 2007 1:22 pm
- Forum: Techniques and Tools
- Topic: How can we make dichroic nametags?
- Replies: 7
- Views: 14451
Re: How can we make dichroic nametags?
I make paw print pendants using a paw print paper punch and the dicro paper. Pain in the neck because the paw is 5 seperate pieces of punch out and you have to place each one just so. The best results are when it is not capped with clear. As far as the names on the glass, could they write them on wi...