Search found 6 matches

by J Campbell
Fri Apr 11, 2003 1:08 pm
Forum: Photos and Stuff
Topic: trying to share
Replies: 4
Views: 11919

Thanks for sharing such cool photos.

Jane
by J Campbell
Mon Apr 07, 2003 2:25 pm
Forum: Photos and Stuff
Topic: Online Fusing Presentation
Replies: 14
Views: 26744

Lisa,

Very nice.....Thank You.

Jane
by J Campbell
Fri Mar 28, 2003 5:27 pm
Forum: Photos and Stuff
Topic: Todays Pot Melt
Replies: 37
Views: 98433

This pot melt technique looks like so much fun. Thank you for showing them.

Jane
by J Campbell
Mon Mar 17, 2003 1:46 pm
Forum: Business Topics
Topic: has anyone ever used an agent?
Replies: 19
Views: 48750

Thank You, for the ideas. I live in Northern CA.

Jane
by J Campbell
Sun Mar 16, 2003 1:18 pm
Forum: Business Topics
Topic: has anyone ever used an agent?
Replies: 19
Views: 48750

I don't think that my last post went through, if it did I'm sorry for posting again!

How does one go about finding a rep? I have tried with no luck. I'm only after one or two. Ideas? Thanks.
by J Campbell
Fri Mar 14, 2003 3:27 pm
Forum: Techniques and Tools
Topic: Buying a Kiln
Replies: 6
Views: 16680

All I can say is get the largest one you can afford. I wish I would have lisen to the advise here myself. Instead, I have one kiln that I don't use and three that I do. Good luck. Jane