Search found 2 matches

by CeaG
Mon Oct 13, 2003 12:35 pm
Forum: Techniques and Tools
Topic: First post...huge bubbles...general glassy despair
Replies: 2
Views: 4353

Thanks for the reply. That's exactly what I wanted to know. My shelf is definitely not gorgeous. Neither side is perfectly flat according to the straightedge test, one side has a slight lip around all edges, and the other side has deep pits and a couple of what look like gouges. I will certainly tal...
by CeaG
Mon Oct 13, 2003 11:27 am
Forum: Techniques and Tools
Topic: First post...huge bubbles...general glassy despair
Replies: 2
Views: 4353

First post...huge bubbles...general glassy despair

I'll attempt to be brief because I know you've all heard this before, but I'm having <yawn> bubble issues. After reading a bazillion posts on the subject and 1)making sure my shelf was thoroughly dry, 2)using the chad trick, and 3)firing excruciatingly slowly, I continued to have problems, so I bega...