Saggar for casting
For my next casting I want to build a ceramic saggar for reinforcement. I've got the Fenton/Kervin book, but I'm still not clear on how it's made. Do you build the ceramic saggar, bisque fire it, then use the saggar as the mold box for the investment casting? If so, will the investment release from ...
- Mon Jan 19, 2004 1:35 pm
- Forum: Photos and Stuff
- Topic: First Combing Attempts
- Replies: 22
- Views: 24765
My glass was firing perfectly until 1700 when I opened the kiln. (This is a kiln that I had the manufacturer make deeper for me so I could make taller vases. Just raising the lid actually turned my one arm red. I had a welder's glove on the other hand and was ready to reach into the kiln but the ex...
- Sun Jan 18, 2004 10:43 pm
- Forum: Business Topics
- Topic: setting up warm glass studio
- Replies: 8
- Views: 12961
Here are a few points to consider: -If your kiln comes with an electric vent, you'll be connecting it a duct that will go to the outside, so be sure you're kiln is within reasonable proximity to an outside wall. -The entire floor doesn't need to be concrete, but it might be advisable to have tile or...
- Sat Jan 17, 2004 2:23 pm
- Forum: Business Topics
- Topic: Sales Tax Audit
- Replies: 3
- Views: 4988
- Sat Jan 17, 2004 1:20 pm
- Forum: Techniques and Tools
- Topic: Question for mud slingers
- Replies: 9
- Views: 9389
Can you be more specific about the problems you are having in drying them? Are they warping, cracking? Why do you keep them sealed in plastic for weeks? In general, you keep clay objects sealed in plastic only while you intend to continue working on them. When a piece is completed, you may wish to c...
- Thu Jan 15, 2004 2:43 pm
- Forum: Techniques and Tools
- Topic: Glass Cut by my Tile Saw
- Replies: 11
- Views: 11253
- Wed Jan 14, 2004 2:03 pm
- Forum: Kiln Casting
- Topic: glass fusion in a sterling silver finding
- Replies: 15
- Views: 19653
Hi Elizabeth! Have you actually tried this yourself? The reason I ask is, I was looking into using Art Clay Silver for the same purpose, to form it as a bezel and backing mount around a glass pendant and put the glass and clay silver back into the kiln. However, I looked through two different books ...
- Wed Jan 14, 2004 1:54 pm
- Forum: Techniques and Tools
- Topic: Glass sticking to ceramic mold.
- Replies: 14
- Views: 17339
- Tue Jan 13, 2004 12:40 pm
- Forum: Techniques and Tools
- Topic: dinnerware
- Replies: 11
- Views: 12117
Well, I tried slumping an oval shaped blank into the mold I built with a rim, and strangely, the mold broke into 2 pieces, while the glass remained in tact. I fired at 300 dph to 1225, hold 45. The mold must have broken during the first segment, since the glass was barely formed. It shows a slight o...
- Mon Jan 12, 2004 10:46 am
- Forum: Techniques and Tools
- Topic: Hi Fire Question
- Replies: 21
- Views: 24228
As for didymium eye protection, nope, wasn't wearing them when I was peaking. I have a pair in the shop, just haven't taken the time to locate 'em. I don't stare at the molten mass, but I do take long glances. You're right tho. I should be more cautious. I was given to understand that didymium glas...
- Fri Jan 09, 2004 4:20 pm
- Forum: Techniques and Tools
- Topic: dinnerware
- Replies: 11
- Views: 12117
I recently completed a mold of an oval shaped platter in which I carved out a rim for the bottom. I'll be firing and then slumping with this mold within the next week, so I'll post how it works out, with greater details if it's successful. I hope it is, because the procedure for making the clay mold...
- Sat Jan 03, 2004 9:52 pm
- Forum: Techniques and Tools
- Topic: Maintaining Geometrical Shapes at Full Fuse
- Replies: 6
- Views: 5965
- Sat Jan 03, 2004 9:27 pm
- Forum: Techniques and Tools
- Topic: Maintaining Geometrical Shapes at Full Fuse
- Replies: 6
- Views: 5965
Maintaining Geometrical Shapes at Full Fuse
I've seen work where geometric shapes like squares, diamonds and rectangles maintain their "perfect" corners or points. Whenever I fuse such shapes in my work, the corners or points always round over some; the only way I've been able to retain the perfect shape is to take it only to a tack...
- Sun Dec 28, 2003 10:41 am
- Forum: Techniques and Tools
- Topic: fiberboard shelflife?
- Replies: 14
- Views: 13275
- Sun Nov 30, 2003 11:13 am
- Forum: Techniques and Tools
- Topic: Distorted Ornaments
- Replies: 11
- Views: 10934
- Tue Nov 25, 2003 11:53 am
- Forum: Techniques and Tools
- Topic: Mold making material
- Replies: 8
- Views: 13085
Low-fire earthenware clay is suitable for making molds; this clay fires at cone 04, around 1900F. Any local pottery supplier will carry it. High fire clay is not necessary, in fact, a lower fired clay mold is less rigid than a high fired one, and can better withstand expansion in the kiln. You can a...
- Thu Nov 20, 2003 2:22 pm
- Forum: Techniques and Tools
- Topic: Distorted Ornaments
- Replies: 11
- Views: 10934
That seems possible. I had made up 3 shelves of ornaments, and in some cases, I was using undiluted glue, and fairly thickly, on others I used a small amount of straight glue, and again on others, the glue was diluted, since I was also applying frit on some ornaments. I'll try a few tests and report...
- Wed Nov 19, 2003 4:03 pm
- Forum: Techniques and Tools
- Topic: Distorted Ornaments
- Replies: 11
- Views: 10934
Distorted Ornaments
Hi folks! I've been making a lot of ornaments recently and some of them distort significantly. E.g., on a 15" shelf, I had one large snowflake (6 triangles, 3 on bottom, 3 overlapped on top) in the centre, and six smaller ones around the perimeter of the shelf. 3 were perfect, the other 3 were ...
- Tue Nov 11, 2003 12:35 pm
- Forum: Techniques and Tools
- Topic: Setting up a warm glass studio.....
- Replies: 40
- Views: 40371
I have a big studio that is not heated and has cement floors (which keeps it cool in summer and unfortunately in winter) so the heat they create is a bonus. Amy Amy, At Home Depot I bought a set of rubber floor mats; these consist of four 2 foot square rubber mats about 1 inch thick, and fit togeth...
- Tue Nov 11, 2003 12:14 pm
- Forum: Techniques and Tools
- Topic: hiding devit
- Replies: 7
- Views: 8067
Velvet Etch works well to etch away devit as well as kiln wash that won't come off the back on Spectrum 96 glass. I usually full fuse again to get back the polish, but recently I was in a hurry and went straight to the slump at 1350F. It was enough to return the glass back its glossy state. Of cours...