Search found 2 matches

by Vicki Shepherd
Mon Aug 12, 2013 12:32 pm
Forum: Techniques and Tools
Topic: Broken sink
Replies: 3
Views: 6896

Re: Broken sink

Actually I do use fiber blanket material...... I use Patty Gray's firing schedule
to fuse the sink so was wondering if I could use the same schedule and just
add time to the soak and annealing times?
by Vicki Shepherd
Mon Aug 12, 2013 10:18 am
Forum: Techniques and Tools
Topic: Broken sink
Replies: 3
Views: 6896

Broken sink

I have a sink that is 5 layers thick of 96. It had one bad side so I have broken it up and want to try and fire it back into the circle. I am using a metal ring with fiber paper lining. I have it in the ring but now have no idea what firing schedule to use. Any ideas? I think it should be held at lo...