Annealing break??

I am trying to use some of my left over glass by fusing them into circles to be used in a future project. I fired a 12" x 3/8" round using the following firing schedule: 275-1150 hold 15 minutes 300-1250 hold 10 minutes 300-1450 hold 3 minutes full to 960 hold 1.30 minutes 50 to 800 hold 2...