Search found 212 matches

by Lisa Allen
Sat Mar 13, 2004 12:53 pm
Forum: Techniques and Tools
Topic: Calendar's Here!!
Replies: 121
Views: 135978

Alecia Helton wrote:Did Lisa ever get hers?

Alecia
Got it!!!! And, love it, you guys are great and much more daring than I.

Lisa
by Lisa Allen
Thu Mar 11, 2004 7:54 pm
Forum: Techniques and Tools
Topic: Calendar's Here!!
Replies: 121
Views: 135978

Another delivery, another day without a calender.............

Ron, if real men work in leather, then real women work with diamonds....at least I got my diamond belt today........

Lisa
by Lisa Allen
Thu Mar 11, 2004 1:59 pm
Forum: Techniques and Tools
Topic: WGW 2004?
Replies: 40
Views: 51285

I'll go where ever the conference goes, name the date and place and I'm there. Can we have another birthday party too? :lol: I promise not to dance on the chair again We can pretend it is my birthday! I for one would be hugely let down if you guys didn't dance on the chairs again. That was a great ...
by Lisa Allen
Thu Mar 11, 2004 12:55 pm
Forum: Techniques and Tools
Topic: WGW 2004?
Replies: 40
Views: 51285

Oh, Asheville sound good too. I like the idea of having it in the south.... As far as an association, I would join in a minute. Member benefits aside, I would just like to help Brad and Jody with the financial and planning issues so that we can keep having the conference annually, without it burdeni...
by Lisa Allen
Thu Mar 11, 2004 1:18 am
Forum: Techniques and Tools
Topic: WGW 2004?
Replies: 40
Views: 51285

WGW 2004?

Just curious if a date and place have been decided on for WGW this year. My vote is still for Chicago coinciding somehow with SOFA, but I would likely go anywhere..... Anyone know anything yet?

Lisa
by Lisa Allen
Wed Mar 10, 2004 9:10 pm
Forum: Techniques and Tools
Topic: Calendar's Here!!
Replies: 121
Views: 135978

Hey Brock, aren't you supposed to be teaching in Atlanta?

Lisa
by Lisa Allen
Wed Mar 10, 2004 2:50 pm
Forum: Techniques and Tools
Topic: Calendar's Here!!
Replies: 121
Views: 135978

Another mail delivery and I am still without a calender.........

If mine got lost somehow, which would not surprise me, are there any left to cover mail losses?

Near gnashing of teeth and rending of garments, Lisa
by Lisa Allen
Wed Mar 10, 2004 2:40 pm
Forum: Techniques and Tools
Topic: Piece Broke While Slumping
Replies: 6
Views: 6880

Any time you have differing thicknesses in a piece, you have to be much more conservative. Also with a consistant 3/8th" thickness, I would have gone up much more slowly, probably 150dph to 1150. But as Charlie said, the nature of the crack will tell you more. If they are rounded then it broke ...
by Lisa Allen
Tue Mar 09, 2004 12:57 pm
Forum: Techniques and Tools
Topic: Calendar's Here!!
Replies: 121
Views: 135978

Just harassed my postman and still NO CALENDER........woe is me.

Lisa
by Lisa Allen
Tue Mar 09, 2004 1:31 am
Forum: Techniques and Tools
Topic: Calendar's Here!!
Replies: 121
Views: 135978

Where is mine??????? I am dying here. Surely I live closer to Chip than PDX Barbara........ My mailman is probably enjoying naked glassies right now along with the front door mat that I never got!

Bummed, Lisa
by Lisa Allen
Fri Mar 05, 2004 7:48 pm
Forum: Techniques and Tools
Topic: Diamond belts for WBS
Replies: 13
Views: 13888

Thanks to all of you! I will check HIS and Abrasive Technology on Monday.

Lisa
by Lisa Allen
Fri Mar 05, 2004 5:20 pm
Forum: Techniques and Tools
Topic: Diamond belts for WBS
Replies: 13
Views: 13888

Diamond belts for WBS

I am running through silicon carbide belts like there is no tomorrow. Does anyone know of a good source for a 60/80 grit diamond belt for a 4"x106" WBS? I need it badly.

Thanks, Lisa
by Lisa Allen
Thu Mar 04, 2004 12:46 pm
Forum: Photos and Stuff
Topic: Sink pictures (only a few of them)
Replies: 35
Views: 41644

Whoa, those are very cool! I'll take the black one with the orangey middle. So, when is the next sink class? I sure would like to be a part of that!

Lisa
by Lisa Allen
Wed Mar 03, 2004 8:39 pm
Forum: Techniques and Tools
Topic: Floral form drape....help!!
Replies: 6
Views: 7950

So, if I have this right, you are trying to drape 2 seperate pieces, one on top of the other, without them fusing together? What temp are you going to? Never done it, but I am guessing that low and long is going to be your best bet, no higher than say 1150 and just hold til you get what you want. Lisa
by Lisa Allen
Fri Feb 27, 2004 4:58 pm
Forum: Techniques and Tools
Topic: Tile Saw
Replies: 26
Views: 27672

Hey Renee- My MK 370 works fine for cutting pattern bars. The only problems with it is that it is quite loud and when I started making thicker and larger slabs, I found it harder to slide the slabs through and get even cuts. But I am making slabs that are 12"x14"x1.5" in depth. If you...
by Lisa Allen
Mon Feb 23, 2004 10:19 pm
Forum: Photos and Stuff
Topic: Puppy Luv
Replies: 9
Views: 12701

She is adorable, Gale!!! I am so glad that she found you. What became of her brothers and sisters?

Lisa
by Lisa Allen
Mon Feb 23, 2004 8:31 pm
Forum: Techniques and Tools
Topic: Popping bubbles?
Replies: 5
Views: 7209

You will probably get some scum inthe pocket from the drilling that you can't get out and the drilled hole will leave a scar as well. The only success I have had drilling a bubble out was to drill it out from the bottom of the piece and re fuse. I had a piece of opaque over clear, so it was easy to ...
by Lisa Allen
Mon Feb 23, 2004 6:02 pm
Forum: Techniques and Tools
Topic: combing/frit?
Replies: 5
Views: 7151

Sure, why not. Give it a try and post the results!

Lisa
by Lisa Allen
Mon Feb 16, 2004 12:07 pm
Forum: Photos and Stuff
Topic: New Photo Setup
Replies: 10
Views: 13525

Paul-
Wow, what a difference a good photo setup makes! I absolutely love Untitled#1. You new direction is really wonderful and these new pics showcase your work beautifully. Kudos!

Lisa
by Lisa Allen
Sat Feb 14, 2004 6:36 pm
Forum: Techniques and Tools
Topic: Frustrating Day with Tile Saw
Replies: 4
Views: 5274

I am not sure which thickness Result blade you are using, but with either, you might try getting some blade stiffeners from HIS. They are just metal discs that go on either side of the blade and give it more rigidity. Also, make sure that you are pushing equally with both hands on the table. I have ...