Search found 32 matches

by Alice DeGraff
Thu Oct 23, 2003 8:48 am
Forum: Photos and Stuff
Topic: The Wine bottles fired from Paradise Paint post Yesterday
Replies: 5
Views: 11627

Hi Tom that looks so neat....

So you slumped the bottle first and then painted it. How high a temp did you need to go with for the paints.... just wondering and how do you like this brand of paint.

Alice De
by Alice DeGraff
Fri Sep 05, 2003 11:18 am
Forum: Photos and Stuff
Topic: Striking pink/dichroic cabs
Replies: 6
Views: 12269

Beautiful.... great job!!! Alice De
by Alice DeGraff
Sat Aug 23, 2003 8:04 am
Forum: Techniques and Tools
Topic: fused glass wall pocket
Replies: 13
Views: 28119

I've made LOTS of wall pockets - I use 2-3 layers of 1/8" fiber paper. The more you use, the slower you have to raise and lower the temp. I have found that the worst breaks happen on the way down, so I take it at 50 dph. I know, it's slooow. but they don't break. On the way up, I start at 75dp...
by Alice DeGraff
Thu Aug 14, 2003 11:58 am
Forum: Photos and Stuff
Topic: New PMC Piece
Replies: 13
Views: 24904

LOVE IT... Alice De
by Alice DeGraff
Thu Aug 14, 2003 11:54 am
Forum: Photos and Stuff
Topic: pate de verre
Replies: 21
Views: 38788

THAT is so beautiful.... Alice De
by Alice DeGraff
Thu Aug 14, 2003 11:32 am
Forum: Techniques and Tools
Topic: outdoor glassblowing studio
Replies: 8
Views: 15947

Ok that is neat. Very organized ! NOW I would like to see the garden !

Alice De
by Alice DeGraff
Thu Aug 14, 2003 11:19 am
Forum: Techniques and Tools
Topic: How do you do it?
Replies: 8
Views: 14963

Thank you so much for bringing this subject up. I too have the problem of doing special orders. I get them then I hate myself for accepting . I love to walk into my studio with no demands on the mind. I love to play, I love to create. After reading the posts I think I have accepted my last "can...
by Alice DeGraff
Thu Aug 07, 2003 1:37 pm
Forum: Photos and Stuff
Topic: Jackie's piece...
Replies: 21
Views: 35989

Wow - sort of surprised to click on here and see my name where I didn't put it. My eyes got big and I thought , "Oh boy - what did I do now" Barbara is right about it being upsidedown, but it was nice of you to post it. I sure would love to see other people's work - any more pictures? I l...
by Alice DeGraff
Thu Jul 31, 2003 7:29 am
Forum: Photos and Stuff
Topic: Something new
Replies: 22
Views: 50238

I felt so relaxed after viewing your work

Alice De
by Alice DeGraff
Tue Jul 29, 2003 2:47 pm
Forum: Photos and Stuff
Topic: Kula Mahina'ai bowl, before slump
Replies: 25
Views: 42373

Kitty wrote:Alice -- LOL! no, not painted.

soooo embarssing :oops: but glad to have given you a good laugh!
by Alice DeGraff
Tue Jul 29, 2003 6:59 am
Forum: Photos and Stuff
Topic: Kula Mahina'ai bowl, before slump
Replies: 25
Views: 42373

i dont know why it wouldnt show up. a friend helped sharpen up my jpeg, which i guess turned it into a bitmap. sorry ... i have no idea how these things work. it's amazing i was able to finally post a picture. Kitty is this blank painted??? I am new to slumping and fusing just wondering.... :oops: ...
by Alice DeGraff
Tue Jul 29, 2003 6:49 am
Forum: Techniques and Tools
Topic: gold leaf/ mica powder
Replies: 49
Views: 87733

Thanks for the tips.. once again, the gold leaf burned up when I sandwiched it between 2 layers ( is going to 1450 too high?) .. oh well.. may try the gold foil. However, I did have success with the mica powder, finally,- applied it very thickly to the underside of clear, then placed on top of blac...
by Alice DeGraff
Mon Jul 28, 2003 6:59 am
Forum: Photos and Stuff
Topic: Kula Mahina'ai bowl, before slump
Replies: 25
Views: 42373

wow that is dreamy.... beautiful....

Alice De \:D/
by Alice DeGraff
Sat Jul 26, 2003 9:53 am
Forum: Photos and Stuff
Topic: Newspaper pix... YOW.
Replies: 8
Views: 16112

Re: Newspaper pix... YOW.

One of my "Blue Cosmos" bowls is displayed in Portland's "Street of Dreams" house showcase. Thursday's newspaper Houses & Gardens of the Northwest pullout section of the Oregonian features the house, "Ambience," which has my Cos on display. If you get the paper, it...
by Alice DeGraff
Sat Jul 26, 2003 9:36 am
Forum: Techniques and Tools
Topic: gold leaf/ mica powder
Replies: 49
Views: 87733

charlie wrote:
Alice DeGraff wrote:Bonnie do you mind sharing Ed Hoy's telephone number???
Thank you Alice De
dags

http://www.edhoy.com/

Darn it they probably dont sell to little guys business oh well maybe I will grow up to a big guy one day thanks for sharing :oops:

Alice De
by Alice DeGraff
Thu Jul 24, 2003 1:29 pm
Forum: Techniques and Tools
Topic: WG@BE3 postponed until 2004
Replies: 22
Views: 35419

[quote="Lani McGregor"]Dear Alice, The new Bullseye Connection Resource Center is (will be) on the East side of the Willamette River (that’s pronounced Will am’ ette, if you ever get here and don’t want native eyes to roll upwards), right next door to the Bullseye Glass factory. Itâ€...
by Alice DeGraff
Thu Jul 24, 2003 1:07 pm
Forum: Techniques and Tools
Topic: gold leaf/ mica powder
Replies: 49
Views: 87733

Thanks for all the input, fellow artisans! Yes, I am using real gold leaf, from Ed Hoy's. I know the fake 'stuff' doesn't work- I had already tried that, too. I use klyr-fire to adhere. ( like a glue) So, today I will try 2 layers of leaf, and no frit to separate the glass, and keep my fingers cros...
by Alice DeGraff
Wed Jul 23, 2003 6:49 am
Forum: Techniques and Tools
Topic: WG@BE3 postponed until 2004
Replies: 22
Views: 35419

Who cares if it is less west or east.... I want to know were it is!!!

Please list where it is. Something new always excites me!

:lol: Alice De
by Alice DeGraff
Tue Jul 22, 2003 7:25 am
Forum: Techniques and Tools
Topic: First Time Art Fair, Looking For Tips
Replies: 23
Views: 37834

OH I forgot one thing.... I freeze my bottle water so it will help keep things cool in the cooler. It melts and then you have a real cold bottle of water to drink :lol:

me again... Alice De
by Alice DeGraff
Tue Jul 22, 2003 7:22 am
Forum: Techniques and Tools
Topic: First Time Art Fair, Looking For Tips
Replies: 23
Views: 37834

ice, ice, ice !!!!! Plus load your things the night before so you can lay awake all night THINKING what did I forget??? Plus if friends want to come over while you are packing SAY NO!!! :oops: :roll:

Alice