by traceynsv
Wed Mar 07, 2018 9:00 pm
Forum: Techniques and Tools
Topic: firing schedule
Replies: 1
Views: 3273

firing schedule

HI All,

I have a water scene that I have already fired, B.E. .clear,with frits size is 12 x 6 Now I want to put that on top of B.E. 4200
do I add more soak time and ramp up slower?

Thanks, Tracey
by traceynsv
Sun Nov 26, 2017 2:30 pm
Forum: Newcomer Forum
Topic: Mold
Replies: 1
Views: 5431

Mold

I bought a earthenware texture tile molds that is an eighth of an inch too big for my kiln how can I fix it
Tracey
by traceynsv
Tue Jun 30, 2015 4:12 pm
Forum: Techniques and Tools
Topic: Kiln running when it's over 95 outside
Replies: 4
Views: 7612

Kiln running when it's over 95 outside

Hi Everyone,

Is it bad to run your kiln (110 V) when its really hot outside?

Thanks,

Tracey
by traceynsv
Tue Jun 09, 2015 3:17 pm
Forum: Techniques and Tools
Topic: kiln elements
Replies: 1
Views: 3074

kiln elements

Does anyone know where I can get an element for a Aim 1407 high fire glass kiln?
Aims customer service is should I say Really Bad!!! To put it nicely

Thanks Tracey
by traceynsv
Fri Jun 22, 2012 5:02 pm
Forum: Techniques and Tools
Topic: Glow in the Dark Powder
Replies: 5
Views: 7752

Re: Glow in the Dark Powder

I guess I was trying to say, How do you seal it between the two glasses, I use clear powder on top, I have also tried just 2 pieces of clear and still got little holes. In other words the top piece of glass was not smooth....
Hope this makes sense.

Thank You so much
by traceynsv
Thu Jun 21, 2012 7:14 pm
Forum: Techniques and Tools
Topic: Glow in the Dark Powder
Replies: 5
Views: 7752

Glow in the Dark Powder

Hi Everyone,

I have been using glow powder and having problems with holes in the glass where the powder is. I know to top with clear, but sometimes I still have holes, thou not all the way through the glass.
Any suggestions?