Re: enamel suggestions

We used a sugary soda pop (Mountain Dew or Coke—not diet, you need the sugar). Open the bottle and let it sit until all of the carbonation is gone. Then mix with glass powder or enamels and spray with your airbrush. It burned out clean and worked great. I suppose you could also just may your own sug...