Search found 3 matches
- Thu Oct 23, 2003 11:02 pm
- Forum: Techniques and Tools
- Topic: Thin fire and scuz
- Replies: 4
- Views: 8021
Thin fire and scuz
In the threads about fiber paper there's been a lot of discussion about pre-firing. I al so know that folks say it's not needed with thin-fire - but many times I get scuz on the edges of pieces with thin fire underneath. Woukd prefiring prevent this? (Or will thin fire crumble under prefiring?)
- Thu Oct 23, 2003 11:00 pm
- Forum: Techniques and Tools
- Topic: Spray A or Boarx between layers
- Replies: 1
- Views: 4406
Spray A or Boarx between layers
If I was going to lay strips of glass at right angles to each other and the particular glass is prone to devitrification, I'd obviously use an overspray. But - must I be super careful to not get any in the "between" places or will it "Mature" there and be OB.
Mary
Mary
- Tue Oct 21, 2003 9:09 am
- Forum: Techniques and Tools
- Topic: Temperature to round edges only
- Replies: 3
- Views: 7017
Temperature to round edges only
I would like to first fire some single sheets of regular bullseye to just round the edges before slumping them in molds, can you tell me a balol park temperature to be looking to slop the processing?