Search found 1 match

by robin g
Sat Dec 15, 2007 12:38 pm
Forum: Techniques and Tools
Topic: How can we make dichroic nametags?
Replies: 7
Views: 14451

Re: How can we make dichroic nametags?

Glassline paints work well for this kind of application also and come in all kinds of colors and with the small tip writing is easy.