Search found 2 matches

by Lisa Sharik
Sun Dec 16, 2007 11:22 pm
Forum: Photos and Stuff
Topic: Large PDV piece
Replies: 2
Views: 6977

Re: Large PDV piece

calico wrote:
what do you do with the little nuggets? they are pretty, but there's no holes so they can't be beads, right?
The people I have sold them to are using wire wrapping techniques to make them into jewelery. I sold the tourmaline ones above 2 hours after I made them 8)
Lisa
by Lisa Sharik
Sat Dec 15, 2007 9:16 am
Forum: Photos and Stuff
Topic: PDV nuggets and slices
Replies: 3
Views: 9321

PDV nuggets and slices

Hi I tried to make my first large piece of pate de verre since class with Marc an Ellen and it didn't turn out as I wanted. So since I had some nice looking glass in an ugly shape I sliced and diced and cold worked it till I took off half of one of my fingernails and abraded both my thumbs #-o The r...