Search found 5 matches

by GetGlassy
Mon Oct 01, 2018 5:50 pm
Forum: Techniques and Tools
Topic: fixing a crack on a tack fused/ slumped piece
Replies: 2
Views: 7611

Re: fixing a crack on a tack fused/ slumped piece

Thanks Brad
I'm going to try. Since it isn't a function piece, I'm going to just try to cover the crack with more frit and stringers.
by GetGlassy
Sun Sep 30, 2018 9:23 am
Forum: Techniques and Tools
Topic: fixing a crack on a tack fused/ slumped piece
Replies: 2
Views: 7611

fixing a crack on a tack fused/ slumped piece

I have a piece that cracked on cool down slump. The crack edges are sharp but only cracked halfway down. The piece is 13x6" 2 layers of clear with bubble powder and powder frit in between full fused. Decorations and frit tack fused on top. It was then slumped on a large stainless steel s-curve....
by GetGlassy
Fri May 16, 2014 3:26 pm
Forum: Techniques and Tools
Topic: Kiln Shelf for a large kiln
Replies: 1
Views: 3210

Kiln Shelf for a large kiln

I am in need of a new shelf for my 42" X 28" kiln. I currently have a fiber board that was treated with hardener. It cracked and has a few gouges that it needs to be replaced. I've researched found vermiculite boards, Kaiser boards, and fiber boards but have no clue on which one might be b...
by GetGlassy
Mon Aug 27, 2012 6:04 pm
Forum: Techniques and Tools
Topic: Pot Melt
Replies: 7
Views: 13758

Re: Pot Melt

That is how I do it Sherry. It adds depth to the pot melt too. I dam mine mainly to keep it contained.
by GetGlassy
Mon Aug 27, 2012 3:37 pm
Forum: Techniques and Tools
Topic: Pot Melt
Replies: 7
Views: 13758

Re: Pot Melt

I've put down a piece of clear in my dam on a kiln washed shelf.