Search found 2 matches
- Sun Dec 16, 2007 11:27 am
- Forum: Newcomer Forum
- Topic: Large Bubbles
- Replies: 4
- Views: 25683
Re: Large Bubbles
I used Spectrum 96 white with Glassline crimson paint for the bottom layer and clear spectrum 96 for the top layer. First I did a paint fuse @ 1100 degrees with no top layer per the instructions from the person who sold me the paint. My second firing schedule for this project was 350 to 1425, hold 2...
- Sun Dec 16, 2007 10:03 am
- Forum: Newcomer Forum
- Topic: Large Bubbles
- Replies: 4
- Views: 25683
Large Bubbles
I am new to the fusing world and have only had minor luck with any glass project. I have started to use fiber paper because kiln wash stuck to the back of the glass and I had large bubbles with break through. This was with single layer glass and frit or smaller pieces. I just tried my first piect wi...