Search found 10 matches
- Tue Aug 05, 2014 12:24 pm
- Forum: Techniques and Tools
- Topic: Tack fuse first?
- Replies: 4
- Views: 6456
Re: Tack fuse first?
It's not necessary to tack fuse everything if your only op intent is to avoid bubbles. After all. The tack fuse isn't a full fuse & so will leave the same bubble-causing spaces! Look up "bubble squeeze" firing schedules and try that, knowing that some bubbles are just unavoidable perio...
- Tue Aug 05, 2014 12:19 pm
- Forum: Techniques and Tools
- Topic: Best Wet Band Sander
- Replies: 8
- Views: 12718
Re: Best Wet Band Sander
I like the CRL / Somaca 104" WBS, BUT it's a large, not inexpensive, floor model.
I switched to it from a table-mounted Covington and saw a world of difference. So if you can stomach that large of a tool, it,s great!
I switched to it from a table-mounted Covington and saw a world of difference. So if you can stomach that large of a tool, it,s great!
- Wed May 21, 2014 6:50 pm
- Forum: Newcomer Forum
- Topic: Does mr97 really need to be reapplied every firing?
- Replies: 7
- Views: 10626
Re: Does mr97 really need to be reapplied every firing?
I use MR-97 for all of my molds and then just a bare kiln shelf with Thinfire for my kiln shelves. I hate the finish that chipped kiln wash leaves on the backs of my pieces... I rarely re-prime the MR-97...recently I draped 18 9" squares over 4 stainless forms...meaning each one was used 4 time...
- Wed May 21, 2014 6:22 pm
- Forum: Techniques and Tools
- Topic: Devitrification in New Kiln/Kiln Shelf
- Replies: 8
- Views: 9661
Devitrification in New Kiln/Kiln Shelf
Hi All, I'm the brand new owner of a Denver kiln and Western Industrial Ceramics 60" x 30" kiln shelf... I did my first test....the very first firing after hooking it up and doing one brief test to 400F. The test involved placing 2" x 2" double-stacked tiles around the kiln...loo...
- Mon Jan 06, 2014 9:25 pm
- Forum: Techniques and Tools
- Topic: Which belt grits?
- Replies: 7
- Views: 9046
Re: Which belt grits?
Like others have said, it depends what you're doing and how you work. I have a large 104" Somaca WBS and use 180 & 220 for almost everything. I can fire polish anything out from 220 grit. Occasionally I'll use a 120. That said, when I was using a much smaller Covington, it seems like I need...
- Fri Dec 27, 2013 3:17 pm
- Forum: Newcomer Forum
- Topic: Sandblasting questions
- Replies: 18
- Views: 29499
Re: Sandblasting questions
Hi All, I too have a larger cabinet-style sandblaster, with factory-supplied dust collector, etc. One, or even several, high-quality water traps are critical to removing all traces of moisture from the air-line. My current setup has two water traps in a row, situated about 2 feet apart and seem to e...
- Mon Dec 23, 2013 3:32 pm
- Forum: Techniques and Tools
- Topic: Removing glass plug from diamond drill bit
- Replies: 25
- Views: 32918
Re: Removing glass plug from diamond drill bit
Order them from these guys. At 35 cents each they are virtually disposable. http://thk.hk/onlinestore_details.php?id=24 I buy all kinds of core bits from them. If these are any good, this is amazing, Rick! I've been spending upwards of $50 each on 1 3/4 diamond hole saws and teirs are $8 with shipp...
- Mon Dec 23, 2013 3:26 pm
- Forum: Techniques and Tools
- Topic: Belt Sander or Lap Wheel
- Replies: 6
- Views: 8098
Re: Belt Sander or Lap Wheel
I agree with all, First the WBS, than a diamond lap.
In my experience, diamonds cut faster & deeper; one often has to use the WBS with t's silicon carbide wet belts in order to remove those fine diamond-produced scratches!
Larry
In my experience, diamonds cut faster & deeper; one often has to use the WBS with t's silicon carbide wet belts in order to remove those fine diamond-produced scratches!
Larry
- Mon Dec 23, 2013 3:14 pm
- Forum: Techniques and Tools
- Topic: Safety relating to thin fire kiln shelf paper
- Replies: 19
- Views: 72738
Re: Safety relating to thin fire kiln shelf paper
Great question/great topic! I would also add in my belief that a mask and gloves, even if latex-free, are not enough protection for any of us glass workers! I use those and vacuum the Thinfire off of the kiln shelf using a HEPA filtered long-handled vacuum. When we brush that dust into a dust pan or...
- Mon Dec 23, 2013 2:33 pm
- Forum: Jewelry Making
- Topic: Tile saws for cutting glass
- Replies: 23
- Views: 64714
Re: Tile saws for cutting glass
I use my MK 101 for the same exact purpose, having migrated to the relatively huge 101 from a smaller MK saw due to my desire to cut much thicker slabs. Beyond price and tool longetivity (and I firmly believe that you get what you pay for...), two issues apply, as follows. 1. The quality of the diam...